Embodiment 1
[0027] The analysis card is made of a cover film 1 and a polydimethylsiloxane color developing substrate 2. The cover film 1 is composed of a non-woven fabric 3 with adhesive backing and an isolation film 4, wherein the material of the isolation film 4 is a poly pair ethylene phthalate; the polydimethylsiloxane color developing substrate 2 is provided with an array of 9 concave cuboid 5 structures, and a reagent module 6 is placed in the cuboid 5, and the reagent module 6 and the instruction manual 8 The discoloration information of the explosive detection reagents is in one-to-one correspondence, and the specific operation is carried out according to the following steps:
[0028] To prepare the polydimethylsiloxane chromogenic substrate:
[0029] a. Place polydimethylsiloxane and peroxide vulcanizing agent in a beaker at a volume ratio of 10:1 and stir until they dissolve evenly to obtain a polydimethylsiloxane solution. After standing for 30 minutes, take 5 ml of polydimethy...
Embodiment 2
[0040] The analysis card is based on Embodiment 1, and the specific operation is carried out according to the following steps:
[0041] To prepare the polydimethylsiloxane chromogenic substrate:
[0042] a. Place polydimethylsiloxane and peroxide vulcanizing agent in a beaker at a volume ratio of 10:1 and stir until they dissolve evenly to obtain a polydimethylsiloxane solution. After standing for 30 minutes, take 5 ml of polydimethylsiloxane. The methylsiloxane solution was slowly poured into the resin-made cuboid template. After standing for 10 minutes, the printed instruction manual 8 was slowly placed on the surface of the polydimethylsiloxane solution, placed for 10 minutes, and then 5ml of polydimethylsiloxane was taken. The base siloxane solution was poured into the cuboid template, placed on the anti-template, and pressed out 9 concave cuboid 5 structures to form an array; then the cuboid template and the anti-template were put into an oven together at a temperature of...
Embodiment 3
[0053] The analysis card is based on Embodiment 1, and the specific operation is carried out according to the following steps:
[0054] To prepare the polydimethylsiloxane chromogenic substrate:
[0055] a. Place polydimethylsiloxane and peroxide vulcanizing agent in a beaker at a volume ratio of 10:1 and stir until they dissolve evenly to obtain a polydimethylsiloxane solution. After standing for 30 minutes, take 5 ml of polydimethylsiloxane. The methylsiloxane solution was slowly poured into the resin-made cuboid template. After standing for 10 minutes, the printed instruction manual 8 was slowly placed on the surface of the polydimethylsiloxane solution, placed for 10 minutes, and then 5ml of polydimethylsiloxane was taken. The base siloxane solution was poured into the cuboid template, put on the anti-template, and pressed out 9 concave cuboid 5 structures to form an array; then put the cuboid template and the anti-template together into an oven, the temperature was 70 °C,...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com