Preparation method of multi-parameter high-throughput sers active microneedle and active microneedle
A high-throughput, multi-parameter technology, applied in the field of biosensing, can solve the problem of not meeting the research needs of acupuncture effect mechanism
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0037] The invention provides a method for preparing a multi-parameter high-throughput SERS active microneedle, the preparation method comprising the following steps:
[0038] 1) Etching grooves on acupuncture needles by means of electrochemical etching, the specific implementation method is:
[0039] 1.1) Soak the acupuncture needles in an insulating polymer solution, and coat the needles of the acupuncture needles with a polymer insulating layer. The insulating polymer solution is polystyrene solution, polypropylene solution, polylactic acid solution or polymethacrylform Ester solution; Acupuncture needles are conventional acupuncture needles used clinically;
[0040] 1.2) Use a razor blade to scratch the polymer insulating layer on the body of the acupuncture needle at a distance of 2-4mm from the acupuncture needle tip, and use it as an etching site for etching the groove;
[0041] 1.3) In the current-time curve mode (0.1-1.5 volt potential), perform electrochemical etchi...
Embodiment 1
[0054] Embodiment 1 Groove etching on acupuncture needles
[0055] Acupuncture needles are soaked in insulating polymers such as 1% polystyrene toluene solution, etc., wrap an insulating layer on the body of the acupuncture needles, and then scratch the insulating layer with a blade as the etching site of the groove. In current-time curve mode (0.1-1.5 volt potential), perform electrochemical etching in 0.5 mol / L sulfuric acid for 5-60 seconds, according to figure 1 Shown etching device (this etching device belongs to prior art), can obtain such as figure 2 Represented grooves.
Embodiment 2
[0056] Embodiment 2 Groove functionalization
[0057] After the acupuncture needles etched with grooves are washed with ethanol, they are soaked in 1% 3-mercaptopropyltriethoxysilane and 3-mercaptopropyltrimethoxysilane ethanol solution for 2-48 hours, and then washed with ethanol Acupuncture needles with grooved thiol can be obtained.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com