A modified resin, raw material composition, preparation method, foaming material and application
A technology of raw material composition and modified resin, which is applied in modified resin, raw material composition, preparation, foaming materials and application fields, can solve problems such as unsatisfactory melt rheological properties, and achieve the benefit of large-scale continuous production Production, high melt elasticity, easy handling effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0080] With the nylon 6 resin of 100 weight parts, the epoxy chain extender of 2.0 weight parts Acrylate polymer and 0.50 parts by weight of antioxidant 1010 are mixed evenly and added to a twin-screw extruder with a rotation speed of 200rpm, melted and blended at 240°C, and the chain-extended nylon 6-1 is obtained by reactive extrusion . The weight-average molecular weight of the chain-extended nylon 6-1 is 32000 g / mol, the molecular weight distribution index is 1.8, and the viscosity is 21000 Pa·s.
Embodiment 2
[0082] The nylon 6 resin of 100 parts by weight, the epoxy chain extender KLE-4370 acrylate polymer of 2.0 parts by weight and the antioxidant 1010 of 0.5 parts by weight, join the twin-screw extruder that rotating speed is 200rpm after mixing uniformly In 240°C, melt blending was carried out, and chain-extended nylon 6-2 was prepared by reactive extrusion. The weight average molecular weight of chain-extended nylon 6-2 is 31000g / mol, the molecular weight distribution index is 1.7, and the viscosity is 20500Pa·s.
Embodiment 3
[0084] With the nylon 6 resin of 100 weight parts, the epoxy chain extender of 2.0 weight parts Acrylate polymer, 3.0 parts by weight of maleic anhydride grafted polypropylene and 0.50 parts by weight of antioxidant 1010 were mixed uniformly and then added to a twin-screw extruder with a rotation speed of 200 rpm, melted and blended at 240 ° C, Long chain branched nylon 6-1 was prepared by reactive extrusion. The weight-average molecular weight of long-chain branched nylon 6-1 is 48000g / mol, the molecular weight distribution index is 2.3, and the viscosity is 75000Pa·s.
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
melting point | aaaaa | aaaaa |
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com