[0025] The present embodiment adopts the following process steps, and its lacquer painting production size is 200 × 100cm, and its formula ratio of color pigment is calculated by mass parts:
[0026] S1. Add 46-58 parts by mass of titanium oxide, 10-12 parts by mass of nickel oxide, 0.78-0.82 parts by mass of barium molybdate, 3-5.4 parts by mass of aluminum oxide, 3.2-5.5 parts by mass of oxide Chromium, 1.1-2.3 parts by mass of potassium soil, 0.8-1.3 parts by mass of barium carbonate, and 0.6-1.1 parts by mass of calcium carbonate are ground into a mixture with a particle size of less than 8 microns by ball milling;
[0027] S2. Add 60-70 parts by mass of synthetic paint to the configuration container, and vibrate and stir with an ultrasonic instrument;
[0028] S3. Pack the fully vibrated and stirred mixture into different sub-containers, respectively add a certain mass of organic mineral colored powder to the sub-containers, the organic mineral colored powder is used, and...
Embodiment 2
[0036] The present embodiment adopts the following process steps, and its lacquer painting production size is 100 × 48cm, and its formula ratio of the color pigment is calculated by mass parts:
[0037] S1. Add 48-55 parts by mass of titanium oxide, 10-11.1 parts by mass of nickel oxide, 0.78-0.82 parts by mass of barium molybdate, 3.5-5.4 parts by mass of alumina, 3.2-4.3 parts by mass of oxide Chromium, 1.1-2.2 parts by mass of potassium soil, 0.8-1.3 parts by mass of magnesium carbonate, and 0.6-1.1 parts by mass of sodium carbonate are ground into a mixture with a particle size of less than 10 microns by ball milling;
[0038] S2. Add 60-70 parts by mass of synthetic paint to the configuration container, and vibrate and stir with an ultrasonic instrument;
[0039] S3. Pack the fully vibrated and stirred mixture into different sub-containers, respectively add a certain mass of organic mineral colored powder to the sub-containers, the organic mineral colored powder is used, ...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com