Silica-gel bionic bait outside coloring method
A bionic bait and silica gel technology, applied in artificial fishing bait, fishing, animal husbandry, etc., can solve the problems of fading, affecting the service life of bionic bait, poor dyeing effect, etc. discoloration effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A method for coloring the exterior of a silicone bionic bait, comprising the following steps:
[0017] (1) Clean the surface of the prepared silicone biomimetic fishing bait, then put it into the modification solution and fully soak it for 3 hours, wherein the modification solution is made of the following components by weight: polyether alkyl modified silicone oil 4 parts, 11 parts of sodium orthovanadate, 140 parts of water;
[0018] (2) In parts by weight, mix 49 parts of methyl methacrylate, 33 parts of butyl acrylate, 14 parts of 3-methoxymethyl acrylate, 38 parts of deionized water, 1 part of emulsifier, and 0.6 parts of initiator After uniformity, heat preservation treatment at 88°C for 3 hours to prepare acrylic emulsion;
[0019] (3) In parts by weight, add 16 parts of promethium chloride and 10 parts of scandium chloride to 130 parts of water, then continue to add 28 parts of sodium naphthenate to it, mix and stir evenly, and raise the temperature of the mixt...
Embodiment 2
[0024] A method for coloring the exterior of a silicone bionic bait, comprising the following steps:
[0025] (1) Clean the surface of the prepared silicone biomimetic fishing bait, then put it into the modification solution and fully soak it for 3.5 hours, wherein the modification solution is made of the following components by weight: polyether alkyl modified silicone oil 5 parts, 13 parts of sodium orthovanadate, 150 parts of water;
[0026] (2) In parts by weight, mix 52 parts of methyl methacrylate, 34 parts of butyl acrylate, 16 parts of 3-methoxymethyl acrylate, 41 parts of deionized water, 2 parts of emulsifier, and 0.8 parts of initiator After uniformity, heat preservation treatment at 90°C for 3.5 hours to obtain an acrylic emulsion;
[0027] (3) In parts by weight, add 18 parts of promethium chloride and 13 parts of scandium chloride to 140 parts of water, then continue to add 32 parts of sodium naphthenate to it, mix and stir evenly, and raise the temperature of t...
Embodiment 3
[0032] A method for coloring the exterior of a silicone bionic bait, comprising the following steps:
[0033] (1) Clean the surface of the prepared silicone bionic bait, then put it into the modification solution and fully soak it for 4 hours, wherein the modification solution is made of the following components by weight: polyether alkyl modified silicone oil 6 parts, 18 parts of sodium orthovanadate, 160 parts of water;
[0034] (2) In parts by weight, mix 55 parts of methyl methacrylate, 36 parts of butyl acrylate, 20 parts of 3-methoxymethyl acrylate, 45 parts of deionized water, 3 parts of emulsifier, and 0.9 parts of initiator After uniformity, the acrylic emulsion was prepared after heat preservation treatment at 92°C for 4 hours;
[0035] (3) In parts by weight, add 20 parts of promethium chloride and 15 parts of scandium chloride to 150 parts of water, then continue to add 36 parts of sodium naphthenate to it, mix and stir evenly, and raise the temperature of the mix...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com