Preparation and use method of multifunctional efficient graphene functional fiber
A functional fiber and graphene technology, applied in fiber type, fiber treatment, biochemical fiber treatment, etc., can solve the problems of high production cost, discount of fiber function, unfavorable production and promotion of functional fiber, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment 1
[0020] Specific embodiment one: the preparation method of multifunctional high-efficiency graphene functional fiber, its steps are:
[0021] (1) After uniformly mixing polyester slices and graphene masterbatch according to the weight ratio of 100:1, graphene polyester fiber is prepared, and the graphene polyester fiber is fluffed, and the fluffed graphene polyester fiber is put into In the polyester mesh bag, the weight of each bag is 4 kg, and the polyester mesh bag is placed on the conveyor belt;
[0022] (2) The polyester mesh bag enters the circulating solution box through the conveyor belt, and the weight ratio of the anti-mite functional additive for textile, the functional additive for textile and water in the solution in the circulating solution box is 1-5:1-5:104 , the temperature of the solution in the circulating solution box is 50 degrees Celsius, and the soaking time of the antibacterial polyester fiber in the circulating solution box is 3-8 minutes;
[0023] (3)...
specific Embodiment 2
[0033] Specific embodiment two: the preparation method of multifunctional high-efficiency graphene functional fiber, its steps are:
[0034] (1) After uniformly mixing polyester chips and graphene masterbatch according to the weight ratio of 100:7, graphene polyester fiber is prepared, and the graphene polyester fiber is fluffed, and the fluffed graphene polyester fiber is put into In the polyester mesh bag, the weight of each bag is 5 kg, and the polyester mesh bag is placed on the conveyor belt;
[0035] (2) The polyester mesh bag enters the circulating solution box through the conveyor belt, and the weight ratio of the anti-mite functional additive for textile, the functional additive for textile and water in the solution in the circulating solution box is 1-5:1-5:104 , the temperature of the solution in the circulating solution box is 50-114 degrees Celsius, and the soaking time of the antibacterial polyester fiber in the circulating solution box is 3-8 minutes;
[0036] ...
specific Embodiment 3
[0046]Specific embodiment three: the preparation method of multifunctional high-efficiency graphene functional fiber, its steps are:
[0047] (1) After uniformly mixing polyester chips and graphene masterbatch according to the weight ratio of 10:1, graphene polyester fiber is prepared, and the graphene polyester fiber is fluffed, and the fluffed graphene polyester fiber is put into In the polyester mesh bag, the weight of each bag is 6.4 kg, and the polyester mesh bag is placed on the conveyor belt;
[0048] (2) The polyester mesh bag enters the circulating solution box through the conveyor belt, and the weight ratio of the anti-mite functional additive for textile, the functional additive for textile and water in the solution in the circulating solution box is 1-5:1-5:104 , the temperature of the solution in the circulating solution box is 114 degrees Celsius, and the soaking time of the antibacterial polyester fiber in the circulating solution box is 3-8 minutes;
[0049] (...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com