Examples
preparation Embodiment 1
[0033] Sodium pyrithione (Hangzhou Wanjing, NPT) 77.6g (0.52mol) was joined in 530g acetone aqueous solution (acetone 20% by weight, water 80% by weight), then added polyhexamethylene guanidine propionate (Shanghai Gao Poly, F3000) 21.0g (0.098mol), polyhexamethylene biguanide hydrochloride (Shanghai Shan's Industrial Co., Ltd., PHMB) 32g (0.146mol) carry out the first mixed contact, and the temperature of contact is 30 ℃, and the time is 10 minutes; then carry out the second mixing contact, the contact temperature is 5°C, and the contact time is 30 minutes; then the solid obtained after the contact is dried and pulverized to obtain the antibacterial agent A1.
preparation Embodiment 2
[0035]Sodium pyrithione (Hangzhou Wanjing, NPT) 64.2g (0.43mol) is joined in 540g acetone aqueous solution (acetone 25% by weight, water 75% by weight), then adds polyhexamethylene guanidine propionate (Shanghai Gao Poly, F3000) 11.1g (0.052mol), polyhexamethylene biguanide hydrochloride (Shanghai Shan's Industrial Co., Ltd., PHMB) 32g (0.146mol) carry out the first mixed contact, and the temperature of contact is 20 ℃, and the time is 15 minutes; then carry out the second mixing contact, the contact temperature is 10°C, and the contact time is 40 minutes; then the solid obtained after the contact is dried and pulverized to obtain the antibacterial agent A2.
preparation Embodiment 3
[0037] Sodium pyrithione (Hangzhou Wanjing, NPT) 64.2g (0.43mol) was joined in 670g acetone aqueous solution (acetone 30% by weight, water 70% by weight), then added polyhexamethylene guanidine propionate (Shanghai Gao Poly, F3000) 15.6g (0.073mol), polyhexamethylene biguanide hydrochloride (Shanghai Shan's Industrial Co., Ltd., PHMB) 32g (0.146mol) carry out the first mixed contact, and the temperature of contact is 40 ℃, and the time is 5 minutes; then carry out the second mixing contact, the contact temperature is 0°C, and the contact time is 60 minutes; then the solid obtained after the contact is dried and pulverized to obtain the antibacterial agent A3.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com