A surface protection method for highly active porous materials
A multi-porous, high-activity technology, applied in the field of material surface protection, can solve the problems that the substrate is easily corroded by the plating solution, the bonding force of the plating layer is not good, rusting or pulverization, etc., to achieve dense crystallization, stable plating solution system, and avoid one-sided effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] A surface protection technology for highly active porous materials is carried out according to the following steps:
[0030] (1) Prepare the sample, using sintered NdFeB as the sample;
[0031] (2) Sample pretreatment, the sample was first degreased in a 50°C degreasing solution for 5 minutes, and then derusted at room temperature for 5 minutes after washing with water. Both degreasing and derusting were carried out with the assistance of ultrasonic waves. The components of degreasing liquid are: 90 g / L NaOH, 0.04 g / L sodium lauryl sulfate aqueous solution. The composition of rust removal solution is: 5% (volume ratio) HNO 3 aqueous solution.
[0032] (3) Immediate impact pre-copper plating, under the action of ultrasonic waves, put the pre-treated and water-washed samples into the cyanide-free copper plating solution at 50°C in a charged way, and the cathode current density is 4 A / dm 2 Impact pre-plating copper for 1min, ultrasonic power is 2W / cm 2 . The compositi...
Embodiment 2
[0037] A surface protection technology for highly active porous materials is carried out according to the following steps:
[0038] (1) Prepare samples, using zinc alloy die-casting materials as samples;
[0039] (2) Sample pretreatment. The sample was first dewaxed in a dewax solution at room temperature for 5 minutes, and then electrochemically degreased for 5 minutes after washing with water. Both dewaxing and degreasing were carried out with the assistance of ultrasonic waves. The wax removal solution is composed of 30% (volume ratio) trichlorethylene solution in ethanol. The components of the degreasing liquid are: 50 g / L NaOH, 0.008 g / L sodium lauryl sulfate aqueous solution, when degreasing, the zinc alloy die casting material is used as the cathode, and the surface area of the zinc alloy die casting material is 2 times larger than that of the zinc alloy die casting material. The graphite plate is used as the anode, and the current density of the cathode is controlle...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com