Dehydrating agent for sludge, and preparation and application thereof
A technology of sludge dewatering agent and aqueous solution, which is applied in the direction of dewatering/drying/concentrating sludge treatment, etc., can solve the problems of low dewatering efficiency of oily sludge and difficulty in oil separation, and achieve high dewatering efficiency, low cost, and reduced land occupation. area effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0037] First, prepare a sludge dewatering agent, the sludge dewatering agent contains the following components in mass percentages: 40% of the inorganic oxide component, 60% of polyacrylamide; the inorganic oxide component contains the following parts by weight Components: 12 parts by weight of silicon dioxide, 3 parts by weight of magnesium oxide, 5 parts by weight of aluminum oxide, and 40 parts by weight of iron oxide.
[0038] (1) mixing each component in the inorganic oxide component according to the proportioning ratio to obtain the inorganic oxide component;
[0039](2) Add polyacrylamide aqueous solution to the inorganic oxide component obtained in the step (1) according to the proportion to obtain the sludge dehydrating agent.
[0040] Then, the prepared sludge dewatering agent is used to dehydrate the oily sludge. The oily sludge is oily biochemical sludge in the petrochemical industry, with a water content of 98% and an oil content of about 10%. Get 200 kilograms o...
Embodiment 2
[0043] First, prepare a sludge dewatering agent, the sludge dewatering agent contains the following components in mass percentages: 38% of the inorganic oxide component, 62% of sodium polyacrylate; the inorganic oxide component contains the following parts by weight Components: 14 parts by weight of silicon dioxide, 2 parts by weight of magnesium oxide, 9 parts by weight of aluminum oxide, and 30 parts by weight of iron oxide.
[0044] (1) mixing each component in the inorganic oxide component according to the proportioning ratio to obtain the inorganic oxide component;
[0045] (2) Adding an aqueous solution of sodium polyacrylate to the inorganic oxide component obtained in step (1) according to the proportioning ratio to obtain a sludge dehydrating agent.
[0046] Then, the prepared sludge dewatering agent is used to dehydrate the oily sludge. The oily sludge is oily anaerobic biochemical sludge in the petroleum industry, with a water content of 95% and an oil content of ab...
Embodiment 3
[0049] First, prepare a sludge dewatering agent, the sludge dewatering agent contains the following components in mass percentages: 32% of the inorganic oxide component, 68% of polyacrylamide; the inorganic oxide component contains the following parts by weight Components: 15 parts by weight of silicon dioxide, 5 parts by weight of magnesium oxide, 6 parts by weight of aluminum oxide, and 60 parts by weight of iron oxide.
[0050] (1) mixing each component in the inorganic oxide component according to the proportioning ratio to obtain the inorganic oxide component;
[0051] (2) Add polyacrylamide aqueous solution to the inorganic oxide component obtained in the step (1) according to the proportion to obtain the sludge dehydrating agent.
[0052] Then, the prepared sludge dewatering agent is used to dehydrate the oily sludge. The oily sludge is oily sludge produced in the process of petroleum smelting, with a water content of 85% and an oil content of about 15%. Get 200 kilogr...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com