Preparation method for bead-like transfer printed fabric
A technology of transfer printing and thermal transfer printing, which is applied in the field of fabric printing, can solve the problems of complex process, high production cost, and no concave-convex three-dimensional effect, and achieve the effect of reducing costs
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A preparation method for imitation sequin transfer printing fabric, comprising the following steps:
[0023] Prepare disperse dyes according to the color of the flower shape, print the transfer paper and dry it at 55°C for 10 minutes to obtain a heat transfer printing paper; hot press the heat transfer printing paper and the engraving film, steam fix and pull out the color, the pressure is 1.5MPa, The temperature is 160°C, and the bonding time is 15 minutes; after the color is pulled out, the engraved film and the thermal transfer printing paper are peeled off and washed to obtain the imitation bead engraving film; the imitation bead engraving film is cut into the required imitation beads by a laser cutting machine Sheet shape, pressing onto the desired fabric, the pressing pressure is 0.8MPa, the temperature is 140°C, and the pressing time is 8 seconds.
[0024] The obtained fabric was washed in a domestic washing machine, and after 300 washing experiments, the imitati...
Embodiment 2
[0026] A preparation method for imitation sequin transfer printing fabric, comprising the following steps:
[0027] Prepare disperse dyes according to the shape and color of the flower, print the transfer paper and dry it at 65°C for 15 minutes to obtain a heat transfer printing paper; hot-press the heat transfer printing paper and the engraving film, steam fix the color, pull out the color, the pressure is 5MPa, the temperature The temperature is 230°C, and the bonding time is 30 minutes; after the color is pulled out, the engraved film and the thermal transfer printing paper are peeled off and washed to obtain the imitation bead engraving film; the imitation bead engraving film is cut into the required imitation bead with a laser cutting machine Shape, pressing onto the desired fabric, the pressing pressure is 1.5MPa, the temperature is 150°C, and the pressing time is 15 seconds.
[0028] The obtained fabric was washed in a domestic washing machine, and after 300 washing exp...
Embodiment 3
[0030] A preparation method for imitation sequin transfer printing fabric, comprising the following steps:
[0031] Prepare disperse dyes according to the color of the flower shape, print the transfer paper and dry it at 60°C for 12 minutes to obtain a heat transfer printing paper; hot press the heat transfer printing paper and the engraving film, steam fix and pull out the color, the pressure is 3.5MPa, The temperature is 200°C, and the bonding time is 25 minutes; after the color is pulled out, the engraved film and the thermal transfer printing paper are peeled off and washed to obtain the imitation bead engraving film; use a laser cutting machine to cut the imitation bead engraving film into the required imitation bead Sheet shape, pressing onto the required fabric, the pressing pressure is 1MPa, the temperature is 145°C, and the pressing time is 10 seconds. According to the shape of the flower, the drilling pressure is 1MPa, the temperature is 150°C, and the drilling time ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com