Dyeing and finishing process of bamboo-cotton blended fabric
A technology of blended fabrics and bamboo cotton, applied in textiles, papermaking, dyeing, plant fibers, etc., can solve the problems of low color fastness and energy consumption of bamboo-cotton blended fabrics, and save dyeing time and cost Low, high dye fastness effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] A kind of dyeing and finishing process of bamboo-cotton blended fabric, comprises the following steps:
[0016] 1) Blanching and bleaching: Prepare bleaching solution, add refining agent, caustic soda, stabilizer, anti-wrinkle agent, hydrogen peroxide into water to make bleaching solution, in which the concentration of refining agent is 1g / L, the concentration of caustic soda is 2g / L, The concentration of the stabilizer is 0.8g / L, the concentration of the anti-wrinkle agent is 1g / L, and the concentration of hydrogen peroxide is 2g / L. The bamboo-cotton blended fabric is put into the bleaching liquid and boiled and bleached at 95°C for 45 minutes;
[0017] 2) Dyeing: Adjust the pH of the bleaching solution to 7, take out the bamboo-cotton blended fabric and put it in the dyeing machine together with the dye solution, add soda ash in an amount of 10g per liter of dye solution, heat the temperature of the dye solution to 90°C and keep it for 20 minutes , the temperature of ...
Embodiment 2
[0022] A kind of dyeing and finishing process of bamboo-cotton blended fabric, comprises the following steps:
[0023] 1) Blanching and bleaching: prepare a bleaching solution, add refining agent, caustic soda, stabilizer, anti-wrinkle agent, and hydrogen peroxide into water to make a bleaching solution, in which the concentration of refining agent is 1.5g / L, and the concentration of caustic soda is 2.5g / L L, the concentration of stabilizer is 0.9g / L, the concentration of anti-wrinkle agent is 1.2g / L,
[0024] The concentration of hydrogen peroxide is 3g / L, and the bamboo-cotton blended fabric is put into the boiling and bleaching liquid, and boiled and bleached at 98°C for 48 minutes;
[0025] 2) Dyeing: Adjust the pH of the bleaching solution to 7, take out the bamboo-cotton blended fabric and put it in the dyeing machine together with the dye solution, add soda ash in an amount of 12g per liter of dye solution, heat the temperature of the dye solution to 92°C and keep it fo...
Embodiment 3
[0030] A kind of dyeing and finishing process of bamboo-cotton blended fabric, comprises the following steps:
[0031] 1) Cooking and bleaching: Prepare a bleaching solution, add refining agent, caustic soda, stabilizer, anti-wrinkle agent, and hydrogen peroxide into water to make a bleaching solution, in which the concentration of refining agent is 2.0g / L, and the concentration of caustic soda is 3g / L , the concentration of stabilizer is 1g / L, the concentration of anti-wrinkle agent is 1.5g / L,
[0032] The concentration of hydrogen peroxide is 4g / L, and the bamboo-cotton blended fabric is put into the boiling and bleaching liquid, and boiled and bleached at 100°C for 50 minutes;
[0033] 2) Dyeing: Adjust the pH of the bleaching solution to 7, take out the bamboo-cotton blended fabric and place it in the dyeing machine together with the dye solution, add soda ash in an amount of 15g per liter of dye solution, heat the dye solution to 95°C and keep it for 30 minutes , the tem...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com