Heat-resistant and flame-retardant modified natural rubber cable sheath material
A technology of natural rubber and cable sheath, which is applied in the direction of insulating cables, rubber insulators, cables, etc., and can solve the problems of threatening life and property safety, unsatisfactory flame retardancy and heat resistance of natural rubber sheath materials, and short service life. , to reduce costs, prevent agglomeration, improve heat resistance and aging resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A kind of heat-resistant flame-retardant modified natural rubber cable sheath material proposed by the present invention, its raw material comprises by weight: 100 parts of natural rubber, 20 parts of nitrile rubber, 35 parts of EPDM rubber, 4 parts of silicon nitrogen rubber , 5 parts of stearic acid, 1 part of magnesium oxide, 2.5 parts of dicumyl peroxide, 2 parts of 1,3,5-trimercapto-2,4,6-s-triazine, 1,1-di-tert-butyl 5 parts of peroxide-3,3,5-trimethylcyclohexane, 5 parts of manganese phosphate, 5 parts of magnesium hydroxide, 5 parts of aluminum hydroxide, 25 parts of modified carbon nanotubes, 10 parts of zirconium diboride, 1 part of anti-aging agent 4010NA, 2.5 parts of accelerator M, 0.8 parts of accelerator TMTD, 8 parts of polybrominated diphenyl ether, 3 parts of trioctyl trimellitate, 5 parts of dimethyl methylphosphonate, polyoxyethylene rosin acid 2 servings.
Embodiment 2
[0018] A kind of heat-resistant flame-retardant modified natural rubber cable sheath material proposed by the present invention, its raw material comprises by weight: 100 parts of natural rubber, 35 parts of nitrile rubber, 20 parts of EPDM rubber, 15 parts of silicon nitrogen rubber , 2 parts of stearic acid, 3 parts of magnesium oxide, 1 part of dicumyl peroxide, 3.5 parts of 1,3,5-trimercapto-2,4,6-s-triazine, 1,1-di-tert-butyl 2 parts of peroxide-3,3,5-trimethylcyclohexane, 10 parts of manganese phosphate, 2 parts of magnesium hydroxide, 12 parts of aluminum hydroxide, 10 parts of modified carbon nanotubes, 20 parts of zirconium diboride, 3 parts of anti-aging agent RD, 1 part of accelerator M, 1.5 parts of accelerator TMTD, 3 parts of polybrominated diphenyl ether, 12 parts of trioctyl trimellitate, 1 part of dimethyl methylphosphonate, 5 parts of polyoxyethylene rosin acid .
Embodiment 3
[0020] A kind of heat-resistant flame-retardant modified natural rubber cable sheath material proposed by the present invention, its raw material comprises by weight: 100 parts of natural rubber, 28 parts of nitrile rubber, 32 parts of EPDM rubber, 10 parts of silicon nitrogen rubber , 3.5 parts of stearic acid, 2 parts of magnesium oxide, 2.2 parts of dicumyl peroxide, 3 parts of 1,3,5-trimercapto-2,4,6-s-triazine, 1,1-di-tert-butyl 4.3 parts of peroxide-3,3,5-trimethylcyclohexane, 7 parts of manganese phosphate, 4 parts of magnesium hydroxide, 8 parts of aluminum hydroxide, 21 parts of modified carbon nanotubes, 18 parts of zirconium diboride, 1 part of anti-aging agent MC, 1 part of anti-aging agent MB, 0.6 part of anti-aging agent RD, 1.8 parts of accelerator M, 1.4 parts of accelerator TMTD, 5.8 parts of polybrominated diphenyl ether, 11 parts of trioctyl trimellitate, methylphosphonic acid 3.2 parts of dimethyl ester, 4 parts of polyoxyethylene rosin acid;
[0021] Wher...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com