A latex paint, healthy technology, applied in latex paint, biocide-containing paint, coating and other directions, can solve the problems of reduced decorative effect and aesthetic effect, affecting people's health, increasing economic burden, etc., to save consumption, odor The effect of softening and reducing the overall cost of painting
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] The invention is a new type of healthy latex paint, which is made of the following raw materials in parts by weight: 5 parts of hollow microsphere emulsion, 15 parts of white latex, 15 parts of titanium dioxide, 5 parts of diatomaceous earth, 2.5 parts of lilialdehyde, 7.5 parts of ionized water, 3.5 parts of dibenzyl biphenol polyoxypropylene polyoxyethylene ether, 1.5 parts of acrylic resin film former and 2.6 parts of ethylene-vinyl acetate copolymer.
[0014] A kind of preparation method of novel healthy latex paint, comprises the following steps:
[0015] 1) Weigh hollow microbead emulsion and white latex according to the above formula, add deionized water and place them together in a stirring tank, and grind and disperse the mixture to a fineness below 5 μm;
[0016] 2) Add the prescribed amount of titanium dioxide and diatomaceous earth into the stirring tank, disperse and stir at 400r / min for 15min, and then heat to 50°C;
[0017] 3) Then weigh lilial and diben...
Embodiment 2
[0020] The invention is a new type of healthy latex paint, which is made of the following raw materials in parts by weight: 10 parts of hollow microsphere emulsion, 25 parts of white latex, 20 parts of titanium dioxide, 10 parts of diatomaceous earth, 6.3 parts of lilial, 8.3 parts of ionized water, 7 parts of dibenzyl biphenol polyoxypropylene polyoxyethylene ether, 4.2 parts of acrylic resin film-forming agent and 4.7 parts of ethylene-vinyl acetate copolymer.
[0021] A kind of preparation method of novel healthy latex paint, comprises the following steps:
[0022] 1) Weigh hollow microbead emulsion and white latex according to the above formula, add deionized water and place them together in a stirring tank, and grind and disperse the mixture to a fineness below 5 μm;
[0023] 2) Add the prescribed amount of titanium dioxide and diatomaceous earth into the stirring tank, disperse and stir at 500r / min for 20min, and then heat to 55°C;
[0024] 3) Then weigh lilial and dibe...
Embodiment 3
[0027] The invention is a new type of healthy latex paint, which is made of the following raw materials in parts by weight: 7 parts of hollow microbead emulsion, 21 parts of white latex, 18 parts of titanium dioxide, 7 parts of diatomaceous earth, 3.8 parts of lilialdehyde, 7.8 parts of ionized water, 5.8 parts of dibenzyl biphenol polyoxypropylene polyoxyethylene ether, 3.2 parts of acrylic resin film-forming agent and 3 parts of ethylene-vinyl acetate copolymer.
[0028] A kind of preparation method of novel healthy latex paint, comprises the following steps:
[0029] 1) Weigh hollow microbead emulsion and white latex according to the above formula, add deionized water and place them together in a stirring tank, and grind and disperse the mixture to a fineness below 5 μm;
[0030] 2) Add the prescribed amount of titanium dioxide and diatomaceous earth into the stirring tank, disperse and stir at 450r / min for 17min, and then heat to 52°C;
[0031] 3) Then weigh lilial and di...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com