Catalyst synthesizing dimethyl oxalate by CO gas phase coupling and preparing method of catalyst
A technology of dimethyl oxalate and catalyst, which is applied to the catalyst for synthesizing dimethyl oxalate by CO gas phase coupling and the field of preparation thereof, and can solve the problems such as the utilization rate of methyl nitrite not being considered.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] carrier modification
[0024] Zirconium tetrachloride (ZrCl 4 ) 0.1025g, add 1mL1:1 (volume ratio) hydrochloric acid solution and 9mL deionized water to make an additive solution, and impregnate α-Al into the solution 2 o 3 20g, after natural drying, roasting at 800°C for 12h, that is, 0.2%ZrO 2 / α-Al 2 o 3 .
[0025] Catalyst preparation
[0026] After adding 0.0851 g of palladium acetate into 10 mL of acetone, ultrasonic treatment was performed for 1 h, followed by light irradiation for 72 h to prepare a palladium acetate / acetone impregnation solution. Then, the solution was impregnated with Zr-modified α-Al 2 o 3 20g, acetone was distilled off after soaking for 6h. Finally, put it into a blast drying oven and dry it at 120°C for 4h, and then reduce it at 300°C for 2h under a hydrogen atmosphere to obtain 0.2%Pd / α-Al 2 o 3 -ZrO 2 catalyst.
[0027] Response Performance Evaluation
[0028] In a fixed-bed reactor with an inner diameter of 12mm and a ...
Embodiment 2
[0030] ZrCl 4 Add 1mL 1:1 (volume ratio) hydrochloric acid solution and 9mL deionized water to 0.1025g to make an auxiliary solution, impregnate 20g of alumina in the solution, dry it naturally, and roast at 1100°C for 8h to obtain 0.2% ZrO 2 / α-Al 2 o 3 .
[0031] Catalyst preparation and reaction performance evaluation are the same as in Example 1.
Embodiment 3
[0033] ZrCl 4 Add 1mL1:1 (volume ratio) hydrochloric acid solution and 9mL deionized water to 0.1025g to make an auxiliary agent solution, impregnate 20g of alumina in the solution, dry it naturally, and roast at 1300°C for 4h to obtain 0.2% ZrO 2 / α-Al 2 o 3 .
[0034] Catalyst preparation and reaction performance evaluation are the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com