[0030] The method for producing cement from urban domestic sewage sludge comprises the following steps:
[0031] 1) Transport 500 kg of domestic sewage sludge from urban sewage treatment plants with a water content of 85% into the mixer, and add 225 kg of gypsum powder into the mixer, mix evenly to make lime gypsum, and transport it to the granulator Make dispersed gray gypsum particles, the particle size of gray gypsum particles is 25-30 mm;
[0032] 2) Send the gray gypsum particles into the far-infrared high-temperature furnace for high-temperature drying at a temperature of 800°C, and send them to the storage bin after cooling;
[0033] 3) Mix 350 kg of gray gypsum particles with 80 kg of slag, 500 kg of cement clinker, and 70 kg of fly ash and stir evenly to form a 1000 kg mixture;
[0034] 4) Send the above-mentioned mixture into a pulverizer for crushing and grinding, and screen through a 820-850 mesh screen to make cement.
[0035] 5) Add the cement and yellow sand m...
Embodiment 2
[0040] The method for producing cement from urban domestic sewage sludge comprises the following steps:
[0041] 1) Transport 500 kg of domestic sewage sludge from urban sewage treatment plants with a moisture content of 90% into the mixer, and add 250 kg of gypsum powder into the mixer, mix evenly to make lime gypsum, and transport it to the granulator Make dispersed gray gypsum particles, the particle size of gray gypsum particles is 15-20 mm;
[0042] 2) Send the gray gypsum particles into the far-infrared high-temperature furnace for high-temperature drying at a temperature of 890°C, and send them to the storage bin after cooling;
[0043] 3) Mix 300 kg of gray gypsum particles with 90 kg of slag, 570 kg of cement clinker, and 40 kg of fly ash and stir evenly to form a 1000 kg mixture;
[0044] 4) Send the above-mentioned mixture into a pulverizer for crushing and grinding, and screen through a 820-850 mesh screen to make cement;
[0045] 5) Add the cement and yellow san...
Embodiment 3
[0049] The method for producing cement from urban domestic sewage sludge comprises the following steps:
[0050] 1) Transport 500 kg of domestic sewage sludge from urban sewage treatment plants with a moisture content of 95% into the mixer, and add 275 kg of gypsum powder into the mixer, mix evenly to make lime gypsum, and transport it to the granulator Make dispersed gray gypsum particles, the particle size of gray gypsum particles is 30-35 mm;
[0051] 2) Send the gray gypsum particles into the far-infrared high-temperature furnace for high-temperature drying at a temperature of 850°C, and send them to the storage bin after cooling;
[0052] 3) Mix 390 kg of gray gypsum particles with 50 kg of slag, 470 kg of cement clinker, and 90 kg of fly ash and stir evenly to form a 1000 kg mixture;
[0053] 4) Send the above-mentioned mixture into a pulverizer for crushing and grinding, and screen through a 820-850 mesh screen to make cement.
[0054] 5) Add the cement and yellow san...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com