Examples
Embodiment 1
[0015] Preparation of high performance additives
[0016] Weigh the raw materials (kg) according to the following proportions:
[0017] 1. BS oil 110, fluorine rubber 12, Siben 80 4, thiadiazole derivatives 7 and chlorobromoalkyl phosphate flame retardant 2;
[0018] 2. BS oil 100, fluorine rubber 15, Siben 80 3, thiadiazole derivatives 8 and chlorobromoalkyl phosphate flame retardant 1;
[0019] 3. High-viscosity synthetic oil 120, fluorine rubber 10, Siben 80 5, thiadiazole derivatives 5 and chlorobromoalkyl phosphate flame retardant 3;
[0020] 4. High-viscosity synthetic oil 105, fluorine rubber 14, Siben 80 3, thiadiazole derivatives 6 and chlorobromoalkyl phosphate flame retardant 2.
[0021] The production method is as follows:
[0022] Add the weighed BS oil or high-viscosity synthetic oil into the reaction kettle, add the weighed fluororubber when the temperature rises to 150°C, stir, continue to heat up to 250°C, keep the temperature until the fluororubber is ...
Embodiment 2
[0024] (1) Add 12 kg of lauryl hydroxystearic acid and 25 kg of mineral oil into the saponification kettle, heat up to the lauryl hydroxystearic acid and start stirring; (2) dissolve 5 kg of lithium hydroxide Form an aqueous solution of lithium hydroxide in water. When the temperature of the mixed solution in step (1) rises to 50-60°C, add the aqueous solution of lithium hydroxide to the saponification kettle; (3) add 4 kg of boric acid to 4 times Dilute with water of boric acid quality, and heat to 85°C to form a boric acid aqueous solution, stir the mixed solution in step (2) for 20 minutes, then add boric acid aqueous solution, continue heating at 90-92°C for saponification reaction for 2-4h; (4) After the saponification reaction is completed, continue to stir and heat up for dehydration. When the temperature reaches 150-160 °C, add 45 kg of mineral oil to keep the temperature for 30 minutes, and continue to heat up to 215-220 °C for 15 minutes, so that the content in the ke...
Embodiment 3
[0026] (1) Add 10 kg of cetyl hydroxy fatty acid and 20 kg of synthetic oil into the saponification kettle, raise the temperature until the cetyl hydroxy fatty acid is dissolved, and start stirring; (2) dissolve 9 kg of lithium hydroxide in water to form hydrogen Lithium oxide aqueous solution, when the temperature of the mixed solution in step (1) rises to 50-60°C, add the lithium hydroxide aqueous solution to the saponification kettle; (3) Add 2 kg of boric acid to 4 times the quality of boric acid in water Dilute and heat to 85°C to form an aqueous solution of boric acid, stir the mixed solution in step (2) for 20 minutes, add the aqueous solution of boric acid, continue heating at 90-92°C for saponification reaction for 2-4 hours; (4) After the saponification reaction is completed , continue to stir and heat up for dehydration. When the temperature reaches 150-160°C, add 45 kg of synthetic oil to keep the temperature for 30 minutes, and continue to heat up to 215-220°C for ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com