[0022] The raw ore of a pegmatite lithium mine in China contains Li 2 O1.52%, the main lithium-containing minerals are spodumene, lepidolite and iron lepidolite, etc., and the main gangue minerals are quartz, plagioclase, microcline, etc.
[0023] The raw ore is crushed and ground to -0.074mm to account for 72%, and the pulp concentration is 40%, then NaOH is added to pH 12 and mechanically stirred and scrubbed for 45 minutes. The pulp after stirring and scrubbing is first concentrated and dehydrated to a pulp concentration of 60%, and then added with clean water to re-adjust the pulp to obtain a pulp concentration of 35% and a pH of 10.
[0024] The ore pulp enters the flotation operation after readjustment, and the flotation operation is one roughing, the second sweeping and the third beneficiation. For the roughing operation, first add 100g / t of benzotriazole, stir for 2 minutes, then add 150g / t of tall oil and stir for 5 minutes, then carry out the roughing operation, and...
Embodiment 2
[0028] The raw ore of a pegmatite lithium ore contains Li 2 O1.05%, the main lithium-containing minerals are spodumene, lepidolite and iron lepidolite, etc., and the main gangue minerals are quartz, feldspar, etc.
[0029] The raw ore is crushed and ground to -0.074mm to account for 80%, and the pulp concentration is 40%, then NaOH is added to pH 12 and mechanically stirred and scrubbed for 45 minutes. The pulp after stirring and scrubbing is first concentrated and dehydrated to a pulp concentration of 58%, and then added with clean water to re-adjust the pulp to obtain a pulp concentration of 38% and a pH of 9. The ore pulp enters the flotation operation after readjustment, and the flotation operation is one roughing, the second sweeping and the third beneficiation. For the roughing operation, first add 80g / t of benzotriazole, stir for 2 minutes, then add 120g / t of tall oil and stir for 5 minutes, then carry out the roughing operation, and the flotation time is 3 minutes; th...
PUM
![No PUM](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/noPUMSmall.5c5f49c7.png)
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com