Electronic product outer shell TPU pearl stereo-molding process
A technology of three-dimensional molding and electronic products, which is applied in the direction of coating, etc., can solve the problems of bad shell feel, high production cost, complicated production process, etc., and achieve the effect of simple production process, low production cost and good softness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0010] The present invention includes PC glue raw material, vulcanizing agent, silicone oil and pearl powder, and is characterized in that: the percentage examples are: PC glue raw material 50%-65%, vulcanizing agent 1%-4%, silicone oil 5%-8%, pearl powder 10% %-35%.
[0011] A processing method of a TPU pearlescent three-dimensional molding process formula for an electronic product shell, the steps are as follows:
[0012] (1) Put the raw material of PC rubber, vulcanizing agent, silicone oil and pearl powder into the mixer and stir evenly for 20-30 minutes to ensure complete fusion. The above ingredients can make the shell piece have good softness.
[0013] (2) Inject the fused ingredients into the mold for molding, the molding temperature is 180-220℃, the injection pressure is controlled at 20-120Mpa, and then baked at 120℃ for 3-4 hours, the appearance has a strong three-dimensional effect and texture. Diversified choices.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com