A water- and oil-repellent, finishing agent technology, used in fiber treatment, textiles and papermaking, animal fibers, etc., can solve the problems of single functional properties, can not fully satisfy customers, and single component composition, and achieve water and oil repellency. The effect of improved performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0009] (1) Heat the temperature of the reaction tank to 68°C, add 2kg of Tween 80, 2kg of emulsifier OP-9, and 2kg of emulsifier OP-20 into the reaction tank after the temperature is reached, and stir evenly with a glass rod; (2 ) Reduce the temperature of the reaction tank to 55°C, then add 5 kg of stearamide and 6 kg of potassium lauryl phosphate into the reaction tank, and stir evenly with a glass rod; (3) Take 3 kg of polyethylene glycol, chlorinate The sodium is 4kg and the water is 260kg. Dissolve polyethylene glycol and sodium chloride in water evenly, pour them into the reaction tank after dissolving, and stir evenly with a glass rod; (4) Cool the mixed liquid to room temperature, and use scissors to The shearing machine is used for shearing treatment, the rotational speed of the shearing machine is 6000 rpm, and the shearing time is 10 minutes. After the shearing is completed, a sweater finishing solution is prepared.
Embodiment 2
[0011] (1) Heat the temperature of the reactor to 58°C, add 3kg of Tween 80, 1kg of emulsifier OP-9, and 2kg of emulsifier OP-20 into the reactor after the temperature is reached, and stir evenly with a glass rod; (2 ) Reduce the temperature of the reactor to 55°C, then add 7kg of stearamide and 5kg of potassium lauryl phosphate to the reactor, and stir evenly with a glass rod; (3) Take 4kg of polyethylene glycol, chlorinate The sodium is 2kg and the water is 275kg. Dissolve polyethylene glycol and sodium chloride in water evenly, pour them into the reaction kettle after dissolving, and stir evenly with a glass rod; (4) Cool the mixed liquid to room temperature, and then use shears to The shearing machine is used for shearing treatment, the rotational speed of the shearing machine is 6000 rpm, and the shearing time is 15 minutes. After the shearing is completed, a sweater finishing solution is prepared.
Embodiment 3
[0013] (1) Heat the temperature of the reactor to 62°C, add 4kg of Tween 80, 2kg of emulsifier OP-9, and 3kg of emulsifier OP-20 into the reactor after the temperature is reached, and stir evenly with a glass rod; (2 ) Reduce the temperature of the reactor to 55°C, then add 6kg of stearamide and 6kg of potassium lauryl phosphate into the reactor, and stir evenly with a glass rod; (3) Take 5kg of polyethylene glycol, chlorinate The sodium is 3kg and the water is 290kg. Dissolve polyethylene glycol and sodium chloride in water evenly, pour them into the reaction kettle after dissolving, and stir evenly with a glass rod; (4) Cool the mixed liquid to room temperature, and use shears to The shearing machine is used for shearing treatment, the rotational speed of the shearing machine is 6000 rpm, and the shearing time is 10 minutes. After the shearing is completed, a sweater finishing solution is prepared.
[0014] Immerse the woolen sweater in the finishing agents prepared in Examp...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com