[0020] (1) Dried honeysuckle dregs to a moisture content of 6%, crushed into powder, and passed through a 60-mesh sieve for later use;
[0021] (2) Add 15g / 100g of corn flour to the above medicinal dregs according to the weight fraction, and mix well;
[0022] (3) Add 20g / 100g of water to the above raw materials according to the weight fraction, and mix well;
[0023] (4) Send the above-mentioned raw materials into a twin-screw extruder for extruding and forming. The screw speed is 190rpm, the feeding speed is 25rpm, and the extrusion temperature is 120°C. Pack and seal to obtain an extruded feed additive.
Embodiment 2
[0025] (1) Dried honeysuckle dregs to a moisture content of 7%, crushed into powder, and passed through a 60-mesh sieve for later use;
[0026] (2) Add 25g / 100g of corn flour to the above medicinal dregs according to the weight fraction, and mix well;
[0027] (3) Add the above raw materials to 17g / 100g of water according to the weight fraction, and mix well;
[0028] (4) Send the above-mentioned raw materials into a twin-screw extruder for extruding and forming. The screw speed is 190rpm, the feeding speed is 25rpm, and the extrusion temperature is 125°C. Pack and seal to obtain an extruded feed additive.
Embodiment 3
[0030] (1) Dried honeysuckle dregs to a moisture content of 8%, crushed into powder, and passed through a 60-mesh sieve for later use;
[0031] (2) Add 35g / 100g of corn flour to the above medicinal dregs according to the weight fraction, and mix well;
[0032] (3) Add the above raw materials to 15 / 100g of water according to the weight fraction, and mix well;
[0033] (4) Send the above-mentioned raw materials into a twin-screw extruder for extruding and forming. The screw speed is 190rpm, the feeding speed is 25rpm, and the extrusion temperature is 130°C. Pack and seal to obtain an extruded feed additive.
PUM
Property | Measurement | Unit |
---|---|---|
weight | aaaaa | aaaaa |
weight | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com