A processing technology and textile technology, applied in the field of mosquito repellent textiles and their processing, can solve the problems of poor fastness, unsuitable for making summer clothing, rough hand feeling on the surface of carrier fabrics, etc., and achieve simple processing technology, strong practicability, Easy-to-use effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] The carrier, permethrin, EDTA and water with a mass ratio of 1:0.1:0.05:100 are mixed and heated to 60°C, and reacted for 36 hours to obtain the mosquito repellent 1, wherein the structure of the carrier is: , Where n is 4.
[0018] Mix 0.01 parts by mass of mosquito repellent 1, 1 part of sodium sulfate and 96.49 parts of water into a finishing solution; put the bleached knitted fabric blank in the finishing solution, and add it after processing at 20°C for 18 minutes The mosquito-repellent fabric can be obtained by soaking 2.5 parts of soda ash for 35 minutes, and finally soaping, washing and drying, and the bath ratio is 1:3. The mosquito-repellent fabric 1 can be produced by using the mosquito-repellent fabric.
Embodiment 2
[0020] The carrier with a mass ratio of 1:0.5:0.01:100, permethrin, EDTA and water are mixed and heated to 80°C, and reacted for 12 hours to obtain the mosquito repellent 2, wherein the structure of the carrier is: , Where n is 8.
[0021] Mix 0.1 parts by mass of mosquito repellent 2, 3 parts of salt and 95.4 parts of water into the finishing solution; put the bleached woven textile blank in the finishing solution, and treat it at 70°C for 10 minutes before adding the mass The mosquito-repellent fabric can be obtained by soaking 1.5 parts of trisodium phosphate for 25 minutes, and finally soaping, washing and drying, and the bath ratio is 1:10. The mosquito-repellent textile 2 can be prepared by using the mosquito-repellent fabric.
Embodiment 3
[0023] The carrier with a mass ratio of 1:0.3:0.03:100, permethrin, EDTA and water are mixed and heated to 70°C, and reacted for 24 hours to obtain the mosquito repellent 3, wherein the structure of the carrier is: , Where n is 6.
[0024] Make up the finishing solution with 0.05 parts by mass of mosquito repellent 3, 2 parts of salt and 95.95 parts of water; put the bleached woven textile blank in the finishing solution, and treat it at 50℃ for 15 minutes before adding the mass The mosquito-repellent fabric can be obtained by soaking 2 parts of trisodium phosphate for 30 minutes, and finally soaping, washing and drying. The bath ratio is 1:6. The mosquito-repellent fabric 3 can be produced by using the mosquito-repellent fabric.
[0025] The mosquito-repellent textiles described in Examples 1-3 have good mosquito-repellent effects when used in mosquito nets.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com