Special high performance environmental-protection type polyurethane waterproof coating material for railway roads and bridges, and preparation method thereof
A polyurethane waterproof, high-performance technology, applied in the direction of polyurea/polyurethane coatings, coatings, etc., can solve problems such as harm to human health, environmental pollution, human health hazards, etc., to achieve safe and environmentally friendly production and use, excellent comprehensive performance, hard work short time effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Preparation of component A: Add 25 parts of polyether TMN3050 (hydroxyl value 56 KOHmg / g) and 45 parts of polyether TDB2000 (hydroxyl value 56 KOHmg / g) into the reactor, heat up to 105°C while stirring, Dehydration at 0.095MPa for 1 hour; then lower the temperature to 62°C. Add 30 parts of MDI-50 and stir evenly, keep it warm at 62°C for 0.5h, then raise the temperature to 84°C, continue to react for 2h until the NCO% value reaches the theoretical value, cool down and discharge the material and seal it for storage, that is, the special high performance for railway bridges Environment-friendly polyurethane waterproof coating A component.
[0024] Preparation of component B: Add 45 parts of YD330N, 35 parts of dimethylthiotoluenediamine, 5 parts of 1000 mesh silica powder, 5 parts of organic montmorillonite, 5 parts of titanium dioxide, and 5 parts of xylene into the reaction kettle, Raise the temperature to 105°C, dehydrate at -0.095Mpa for 2 hours; then cool down to be...
Embodiment 2
[0027] Preparation of component A: Add 40 parts of polyether TMN3050 (hydroxyl value 56 KOHmg / g) and 20 parts of polyether TDB2000 (hydroxyl value 56 KOHmg / g) into the reactor, heat up to 105°C while stirring, Dehydration at 0.095Mpa for 1 hour; then lower the temperature to 62°C. Add 40 parts of MDI-50 and stir evenly, keep warm at 62°C for 0.5h, then raise the temperature to 84°C, continue to react for 2h, until the NCO% value reaches the theoretical value, cool down and discharge the material and seal it for storage, that is, the high performance special for railway bridge Environment-friendly polyurethane waterproof coating A component.
[0028]Preparation of component B: Add 70 parts of YD330N, 15 parts of dimethylthiochlorophenylenediamine, 3 parts of 1000 mesh silica powder, 5 parts of organic montmorillonite, 2 parts of titanium dioxide, and 5 parts of xylene into the reaction kettle , heat up to 105°C, dehydrate at -0.095Mpa for 2 hours; then cool down to below 65°C,...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com