A production process, polyester cotton technology, applied in dyeing method, continuous processing of textile materials, heating/cooling of fabrics, etc., can solve the problems of non-compliance with environmental protection requirements, large water, electricity and steam consumption, complicated process, etc., and achieve bright color , save energy consumption, reduce the effect of process flow
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] Embodiment 1, described a kind of polyester-cotton dyeing same-bath method manufacturing process, carries out according to the following steps:
[0023] 1) Use gray cloth of polyester-cotton (or cotton-polyester) blended fabric for distribution;
[0024] 2) Cold pile: In the process of cold pile, the water temperature is first heated to 30-40 0 C. Add the following additives in order according to the amount of water, that is, add per liter of water: Add chelating agent (K10 water quality agent) 2g / l at a uniform speed within 5-10 minutes; Add liquid caustic soda (sodium hydroxide) 50g / l at a constant speed within 5-10 minutes; Add refining agent (sodium dodecylsulfonate) 3g / l at a uniform speed within 5-10 minutes; Add hydrogen peroxide 3g / l at a constant speed within 5-10 minutes; Add stabilizer 2g / l uniformly within 5-10 minutes; Add degreasing agent (sodium fatty alcohol sulfate) 3g / l at a uniform speed within 5-10 minutes;
[0025] 3), stacked for 24 hou...
Embodiment 2
[0034] Embodiment 2, described a kind of polyester-cotton dyeing same-bath method manufacturing process, carries out according to the following steps:
[0035] 1) Use gray cloth of polyester-cotton (or cotton-polyester) blended fabric for distribution;
[0036] 2) Cold pile: In the process of cold pile, the water temperature is first heated to 30-40 0 C. Add the following additives in order according to the amount of water, that is, add per liter of water: Add chelating agent (K10 water quality agent) 3g / l at a uniform speed within 5-10 minutes; Add liquid caustic soda (sodium hydroxide) 80g / l at a uniform speed within 5-10 minutes; Add refining agent (sodium dodecylsulfonate) 6g / l at a uniform speed within 5-10 minutes; Add hydrogen peroxide 6g / l at a constant speed within 5-10 minutes; Add stabilizer 3g / l uniformly within 5-10 minutes; Add degreasing agent (sodium fatty alcohol sulfate) 5g / l at a uniform speed within 5-10 minutes;
[0037] 3), stacked for 24 hour...
PUM
![No PUM](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/noPUMSmall.5c5f49c7.png)
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com