Manufacturing method of papermaking sewage type cationic polyacrylamide
A technology of polyacrylamide and paper-making sewage, which is applied in the field of paper-making sewage-type cationic polyacrylamide, can solve the problems of unreachable, backward technology, high price, etc., and achieve high stability, good adsorption and high purity.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Initiating system A is firstly added to the mixture of acrylamide and cationic monomer, and then adding initiating system B, using vertical reactor equipment at normal temperature and pressure, reacting for 0.5 hours to 2 hours to form a transparent gel, and then through Aging at 80-95°C for 0.5 hours to 2 hours, after the process of granulation→salting out→drying→crushing→screening→packaging, the ionicity is between 20%-30%, and the molecular weight is 8-12 million. Cationic polyacrylamide products with an apparent viscosity greater than 40cP; adding the initiator system A to the mixed solution is an azo chemical, V40, V44 and V50, the amount added is 0.001 times the weight of the mixed solution, and the initiator system is added to the mixed solution B is an oxidizing agent and a reducing agent. The oxidizing agent is potassium persulfate and sodium persulfate, and the reducing agent is sodium sulfite and sodium bisulfite. The addition of these two reagents is 0.000008...
Embodiment 2
[0015] Initiating system A is firstly added to the mixture of acrylamide and cationic monomer, and then adding initiating system B, using vertical reactor equipment at normal temperature and pressure, reacting for 0.5 hours to 2 hours to form a transparent gel, and then through Aging at 80-95°C for 0.5 hours to 2 hours, after the process of granulation→salting out→drying→crushing→screening→packaging, the ionicity is between 20% and 30%, the molecular weight is 8-12 million, and the apparent Cationic polyacrylamide products with a viscosity greater than 40cP; adding initiator system A to the mixed solution is an azo chemical, V59 and V60, and the amount added is 0.002 times the weight of the mixed solution; adding initiator system B to the mixed solution is an oxidizing agent and reducing agent, the oxidizing agent is potassium persulfate, sodium persulfate and ammonium persulfate, the reducing agent is sodium pyrosulfate and ferrous ammonium sulfate, and the addition of these t...
PUM
Property | Measurement | Unit |
---|---|---|
Apparent viscosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com