Preparation method and application for magnetic molecularly imprinted polymers for selectively separating carbamazepine
A magnetic molecular imprinting and polymer technology, which is applied in the preparation of test samples, alkali metal compounds, chemical instruments and methods, etc., can solve the problems of cumbersome dynamic separation operation, limited application range, and difficult separation, and achieve simplified samples Processing process, expanding the scope of application, good selectivity effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0040] The synthesis method of the magnetic molecularly imprinted polymer selectively adsorbing carbamazepine of the present invention is as follows:
[0041] (1) Synthesis of magnetic chitosan nanoparticles: fully dissolve 0.5 g chitosan in 50 mL 3% (v / v) acetic acid aqueous solution, and add 0.2 g Fe 3 o 4 , Ultrasonic dispersion for 30min. After stirring mechanically for 5 min in a constant temperature water bath at 20-30 °C, add 40 mL of liquid paraffin and 0.5 mL of Span 80 in sequence, and use 25% (v / v) NH 3 ·H 2 O aqueous solution was used to adjust the pH of the solution to 8, and finally 1ml of 25% (v / v) glutaraldehyde solution was added, and the temperature was raised to 50°C for 2 hours. After the reaction, the synthesized magnetic chitosan nanoparticles (chitosan-Fe 3 o 4 ), separated by a permanent magnet, washed repeatedly with absolute ethanol and deionized water for 10 times, and then vacuum-dried at 40°C for later use.
[0042] (2) Pre-assembly solution:...
Embodiment 2
[0056] The synthesis method of the magnetic molecularly imprinted polymer selectively adsorbing carbamazepine of the present invention is as follows:
[0057] (1) Synthesis of magnetic chitosan nanoparticles: fully dissolve 0.5g chitosan in 100mL 3% (v / v) acetic acid solution, and add 0.5g Fe 3 o 4 , Ultrasonic dispersion for 30min. After stirring mechanically for 5 min in a constant temperature water bath at 20-30 °C, add 10 mL of liquid paraffin and 0.5 mL of Span 80 in sequence, and use 25% (v / v) NH 3 ·H 2 O aqueous solution was used to adjust the pH of the solution to 9, and finally 3ml of 25% (v / v) glutaraldehyde solution was added, and the temperature was raised to 60°C for 2 hours. After the reaction, the synthesized magnetic chitosan nanoparticles were separated with a permanent magnet, washed repeatedly with absolute ethanol and deionized water for 15 times, and vacuum-dried at 40°C for future use.
[0058] (2) Pre-assembly solution: Weigh 75.6 (0.32 mmol) carbama...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Saturation magnetization | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com