A technology of real stone paint and imitation granite, which is applied in the direction of antifouling/underwater paint, coating, paint containing biocide, etc., can solve the problems of single color of real stone paint and heavy weight of granite marble, etc., and achieve strong three-dimensionality and color Rich, realistic effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] An imitation granite real stone coating, in terms of percentage by weight, is composed of the following components: 6% of deionized water, 6% of 2% hydroxyethyl cellulose solution (30,000 viscosity); F111 defoamer 0.15%; LXE antiseptic bactericide 0.1%; AMP-95 multifunctional auxiliary agent 0.3%; (40~80) mesh quartz sand 28%; (80~120) mesh quartz sand 50%; colored rock chips 4% ; XG-60 thickener 1.45%.
[0027] Its preparation method: take 4% of deionized water by weight, add 2% hydroxyethyl cellulose solution (30,000 viscosity) 6% in turn; 4% of alcohol lipid 12 film-forming aids, whichever is film-forming; F111 Defoamer 0.15%; LXE antiseptic bactericide 0.1%; AMP-95 multifunctional additive 0.3%, adjust pH 8~9 is appropriate; (40~80) mesh quartz sand 28%; (80~120) mesh quartz sand 50 %; colored rock flakes 4%; water replenishment 2%; XG-60 thickener 1.45%, and then the above-mentioned raw materials are mixed uniformly to obtain the imitation granite real stone coati...
Embodiment 2
[0029] A kind of imitation granite real stone coating, according to the weight percentage, is composed of the following components: deionized water 6%, 2% hydroxyethyl cellulose solution (30,000 viscosity) 6%; F111 Defoamer 0.15%; LXE Antiseptic Bactericide 0.1%; AMP-95 Multifunctional Auxiliary 0.3%; (40~80) Mesh Quartz Sand 39%; (80~120) Mesh Quartz Sand 39%; ; XG-60 thickener 1.45%.
[0030] Its preparation method is the same as claim 1.
Embodiment 3
[0032] An imitation granite real stone coating, in terms of weight percentage, is composed of the following components: deionized water 6%, 2% hydroxyethyl cellulose solution (30,000 viscosity) 6%; F111 defoamer 0.15%; LXE antiseptic bactericide 0.1%; AMP-95 multifunctional auxiliary agent 0.3%; (40~80) mesh quartz sand 50%; (80~120) mesh quartz sand 28%; colored rock chips 3% ; XG-60 thickener 1.45%.
PUM
Property | Measurement | Unit |
---|---|---|
viscosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com