Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Anti-creasing agent

A technology of anti-wrinkle agent and softener, applied in the field of anti-wrinkle agent, can solve problems such as skin damage, uncomfortable wearing, loss of effect, etc., and achieve the effect of low cost and simple preparation process

Inactive Publication Date: 2012-05-23
CHENGDU SHUNFA DISINFECTANT & WASHING TECH
View PDF1 Cites 3 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0005] 1. The anti-wrinkle agent is added when the fabric is produced, and it will lose its effect after wearing it for a long time;
[0006] 2. After adding the anti-wrinkle agent, the texture of the clothes is hard, uncomfortable to wear, and harmful to the skin;

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] An anti-wrinkle agent, comprising the following components in parts by weight:

[0028] Aluminum acetate 5 parts

[0029] Aminated epoxy resin 10 parts

[0030] Polyethylene glycol oleyl ether 5 parts

[0031] Cationic softener 10 parts

[0032] Lactic acid 2 parts

[0033] Potassium hydroxide 1 part

[0034] 200 parts of water.

[0035] Described anti-wrinkle agent is made by following method:

[0036] Mix all the raw materials into water, stir evenly, heat to 50°C, keep it warm for 3 hours, and get the anti-wrinkle agent after cooling to room temperature.

Embodiment 2

[0038] An anti-wrinkle agent, comprising the following components in parts by weight:

[0039] Aluminum acetate 15 parts

[0040] Aminated epoxy resin 20 parts

[0041] Polyethylene glycol oleyl ether 8 parts

[0042] 20 parts of non-ionic softener

[0043] Lactic acid 8 parts

[0044] Potassium hydroxide 5 parts

[0045] 500 parts of water.

[0046] Described anti-wrinkle agent is made by following method:

[0047] Mix all the raw materials into water, stir evenly, heat to 70°C, keep it warm for 7 hours, and get the anti-wrinkle agent after cooling to room temperature.

Embodiment 3

[0049] An anti-wrinkle agent, comprising the following components in parts by weight:

[0050] Aluminum acetate 10 parts

[0051] Aminated epoxy resin 15 parts

[0052] Polyethylene glycol oleyl ether 6 parts

[0053] Anionic softener 15 parts

[0054] Lactic acid 5 parts

[0055] Potassium hydroxide 3 parts

[0056] 350 parts of water.

[0057] Described anti-wrinkle agent is made by following method:

[0058] Mix all the raw materials into water, stir evenly, heat to 60°C, keep it warm for 5 hours, and get the anti-wrinkle agent after cooling to room temperature.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to an anti-creasing agent, more specifically to an anti-creasing agent for clothes. The anti-creasing agent contains the following components of: by weight, 5-15 parts of aluminum acetate, 10-20 parts of an aminated epoxy resin, 5-8 parts of polyethylene glycol oleyl ether, 10-20 parts of a softening agent, 2-8 parts of lactic acid, 1-5 parts of potassium hydroxide, and 200-500 parts of water. The anti-creasing agent provided by the invention has advantages of full function, simple preparation technology and low cost, and is applicable to be widely used at home.

Description

technical field [0001] The present invention relates to an anti-wrinkle agent, more particularly, the present invention relates to an anti-wrinkle agent for clothes. Background technique [0002] In the existing technology, there is a process in the processing of ready-made garments, which is to add anti-wrinkle agent, so that it will play an anti-wrinkle effect when wearing clothes at ordinary times, but after wearing for a long time, the anti-wrinkle agent will lose its effectiveness. Wrinkles will appear on the clothes, affecting the wearing comfort and appearance. [0003] The application number is 200810234620.6, and the invention patent titled "An anti-wrinkle agent for cellulose fiber fabrics and its synthesis method" discloses a kind of anti-wrinkle agent for cellulose fiber fabrics. Its general structural formula is as above, In the formula, 5≤A≤20, 0≤B≤20, 0≤C≤20, 0≤D≤10, 40≥A+B+C+D≥10, B, C and D are not 0 at the same time; the average Molecular weight M n ≥130...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): D06M15/55D06M13/188D06M15/53D06M13/207D06M11/38
Inventor 梁宗贵
Owner CHENGDU SHUNFA DISINFECTANT & WASHING TECH
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products