Embodiment 1
[0019] A double-layer structure antistatic polyvinyl chloride plastic floor is characterized in that it is composed of a double-layer structure, the auxiliary material forms the surface layer, and the main material forms the bottom layer; in parts by weight,
[0020] The main material formula is: polyvinyl chloride resin 100kg, tribasic lead sulfate 8kg, kaolin 200kg, dipentaerythritol 25kg, carbon black 5kg, dibutyl phthalate 4kg, ethoxylated aliphatic alkylamine 5kg, paraffin wax 10kg;
[0021] The formula of auxiliary materials is: 100 kg of polyvinyl chloride resin, 10 kg of MBS resin, 3 kg of zinc stearate, 4 kg of dibutyl phthalate, 5 kg of tribasic lead sulfate, and 2 kg of di-tert-butyl hydroquinone resin.
[0022] A preparation process for a double-layer structure antistatic polyvinyl chloride plastic floor:
[0023] A, mixing mix the above formula;
[0024] B. Mixing: Plasticize the PVC evenly on the two-roll plastic refining machine; the temperature is about 140-1...
Embodiment 2
[0029] A double-layer structure antistatic polyvinyl chloride plastic floor is characterized in that it is composed of a double-layer structure, the auxiliary material forms the surface layer, and the main material forms the bottom layer; in parts by weight,
[0030] The main material formula is: polyvinyl chloride resin 120kg, tribasic lead sulfate 10kg, kaolin 250kg, dipentaerythritol 30kg, carbon black 10kg, dibutyl phthalate 6kg, ethoxylated aliphatic alkylamine 10kg, paraffin wax 10kg;
[0031] The formula of auxiliary materials is: 120kg of polyvinyl chloride resin, 12kg of MBS resin, 5kg of zinc stearate, 6kg of dibutyl phthalate, 8kg of tribasic lead sulfate, and 4kg of di-tert-butylhydroquinone resin.
[0032] A preparation process for a double-layer structure antistatic polyvinyl chloride plastic floor:
[0033] A, mixing mix the above formula;
[0034] B. Mixing: Plasticize the PVC evenly on the two-roll plastic refining machine; the temperature is about 140-160; ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com