Production method of natural colored cotton, ramie and white cotton fiber blended yarn
A technology of fiber blending and production methods, applied in the direction of yarn, textiles and papermaking, etc., can solve the problems of residual harmful chemical components and overall grade reduction of finished products, achieve good economic and social benefits, improve grades, and avoid chemical residues.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0010] The preparation method of the present invention is the following steps:
[0011] ①. Blowing, carding, pre-drawing, coiling and combing of 2-4 natural colored cotton fibers of different colors are carried out respectively. , strong carding" as the process route, the cleaning beater is below 500r / min, the carding cylinder speed is 320r / min, the licker-in roller speed is 750r / min, the doffer speed is 18r / min, the sliver weight is 40-45g / m, combed Quantitative 16-18g / 5m;
[0012] ②. The ramie is cleaned, carded, and pre-drawn. The carding weight is 16-18g / 5m, the pre-drawing weight is 15-17.5g / 5m, the carding cylinder speed is 360r / min, and the licker-in speed is 800r / min , doffer speed 20r / min;
[0013] 3. The obtained fiber strips of different colors are drawn respectively with ramie fibers (three passes), roving, spun yarn, winding, and finally several bobbins of different colors are obtained, and the spun yarn twist coefficient is 290-390;
[0014] The natural colore...
Embodiment 1
[0016] Embodiment one batching: green natural color cotton 20%, white cotton 40%, ramie 40%;
[0017] Preparation:
[0018] ①. The natural colored cotton fiber is processed by cleaning, carding, pre-drawing, sliver coiling, and combing respectively. When opening and striking, the process is "light weight, slow speed, tight gauge, and strong carding" Route, cleaning beater below 500r / min, carding cylinder speed 320r / min, licker-in speed 750r / min, doffer speed 18r / min, sliver weight 40-45g / m, combing weight 16-18g / 5m;
[0019] ②. The ramie is cleaned, carded, and pre-drawn. The carding weight is 16-18g / 5m, the pre-drawing weight is 15-17.5g / 5m, the carding cylinder speed is 360r / min, and the licker-in speed is 800r / min, doffer speed 20r / min;
[0020] 3. The obtained fiber strips of different colors are drawn respectively with ramie fibers (three passes), roving, spun yarn, winding, and finally several bobbins of different colors are obtained, and the spun yarn twist coefficie...
Embodiment 2
[0022] Ingredients: 30% of green or brown or yellow or red natural colored cotton, 40% of ramie, 30% of white cotton... The preparation method is the same as that of Example 1.
[0023] In summary, the blended yarn of natural colored cotton and ramie fiber of the present invention has natural color and luster, does not need to be dyed after weaving, has no chemical residues, enriches the color varieties of ramie fabrics, and improves the product quality. production value.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com