Construction method for water stop belt for moisture-proof water stop
A construction method and waterstop technology, applied in the field of construction, can solve the problems of long construction period, easy deformation, cumbersome vertical shell formwork, etc., and achieve the effects of shortening the construction period, stable quality, and saving labor and materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] Embodiment 1, the high-grade concrete solid brick of the present invention and special cement can make finished product in factory in advance. Among them, the proportion of high-grade concrete solid bricks is (by weight): 30 parts of ordinary 32.5R Portland cement, 40 parts of stones (3-10mm in particle size), 20 parts of yellow sand (medium-coarse is better) , 1 part of water reducing agent (such as polycarboxylic acid series water reducing agent), 1 part of waterproofing agent (such as silicone waterproofing agent), mix and stir all the raw materials, and place them in the concrete forming machine to make concrete solid bricks. The proportion of special cement is (by weight): 45 parts of low-alkali sulfoaluminate cement, 45 parts of fine sand, 1 part of water-repellent (such as silicone water-repellent), water-reducing agent (such as polycarboxylic acid series water-repellent) 1 part of water agent), 0.1 part of hydroxypropyl methylcellulose, 0.1 part of redispersible...
Embodiment 2
[0014] Embodiment 2, the construction method of this example and example 1 is the same, only the raw material ratio of high-grade concrete solid brick and special mortar is different. Among them, the proportion of high-grade concrete solid bricks is (by weight): 25 parts of ordinary 42.5R Portland cement, 50 parts of gravel (3-10mm in particle size), 25 parts of yellow sand (medium coarse), water-reducing 3.5 parts of water-repellent, 4.5 parts of waterproofing agent; the proportion of special cement is (by weight): 35 parts of low-alkali sulfoaluminate cement, 60 parts of fine sand, 4.5 parts of waterproofing agent, 3.5 parts of water-reducing agent, hydroxypropyl 0.3 parts of methyl cellulose, 0.55 parts of redispersible latex powder, and 0.55 parts of air-entraining agent.
Embodiment 3
[0015] Embodiment 3, the construction method is the same as Example 1, wherein, the proportioning of the high-grade concrete solid brick is (by weight): 20 parts of ordinary 52.5R Portland cement, 60 parts of stones (3-10mm in particle size), 60 parts of yellow 30 parts of sand (medium coarse), 6 parts of water reducing agent, 8 parts of waterproofing agent; the proportion of special cement is (by weight): 25 parts of low-alkali sulfoaluminate cement, 75 parts of fine sand, 8 parts of waterproofing agent 1 part, 6 parts of water reducer, 0.5 part of hydroxypropyl methylcellulose, 1 part of redispersible latex powder, 1 part of air-entraining agent.
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com