[0026] A kind of production method of porcelain whole body antique brick of the present invention, comprises following method step:
[0027] (1) make the adobe of archaize brick, comprise following method step:
[0028] ①According to weight percentage: 68-75% silicon dioxide, 15-22% aluminum oxide, 2.0-3.5% potassium monoxide, 2.0-3.8% disodium oxide, 0.35-0.9% iron oxide , 0.005-0.15% titanium oxide, 0.1-0.75% calcium oxide and 0.4-1.0% magnesium oxide, each of which requires a whiteness of 60 degrees and a loss on ignition of 5%;
[0029] ②Mix the obtained ingredients evenly to obtain the required mixture;
[0030] ③Put the obtained mixture into the ball milling equipment and ball mill it into a slurry. The ball milling time is 12-13 hours. The slurry concentration requirement: the moisture content should be controlled at 30-32%. Sieve (that is, a wet vibrating sieve with an aperture of 0.28 mm) is screened and put into the slurry tank to obtain a slurry that meets the req...
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com