[0023] 3% cyclohexanone, 20% ethyl salicylate, 10% butyl salicylate, 45% No. 100 gasoline, made into a solvent, put into a container and stir, add 22% polystyrene foam, and then Stir, grind, and filter to make the finished product.
Embodiment 2
[0025] Cyclohexanone 6%, ethyl salicylate 12%, butyl salicylate 15%, No. 120 gasoline 42%, dubbed as solvent. After being put into a container and stirred, add 25% of polystyrene foam, add 8% lithopone filler of the total amount of the above raw materials, and then stir, grind, and filter to make a finished product. Pour it into a container made of iron sheet and seal it according to the regulations.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com