Fibroin sunscreen cream and preparation method thereof
A technology of silk protein and sunscreen, applied in the field of daily chemicals, can solve problems such as poor moisturizing effect, achieve the effects of not easily lost, improve moisturizing effect, and solve moisturizing antagonistic effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0029] A preparation method of silk protein sunscreen, the specific preparation steps comprising:
[0030] Preparation of the water phase:
[0031] In parts by weight, 100-200 parts of water, 10-20 parts of glycerin, 8-10 parts of graphene oxide, 3-5 parts of dopamine, and 8-10 parts of silk protein are sequentially taken;
[0032] After mixing water, glycerin and silk protein, ball mill for 4-6 hours to obtain ball mill;
[0033] Add graphene oxide and dopamine to the ball mill, and after ultrasonic dispersion, continue ball milling and mixing for 3-5 hours to obtain the aqueous phase;
[0034] Product formulation:
[0035] In parts by weight, take 10-20 parts of oil phase, 60-80 parts of water phase, and 3-5 parts of emulsifier, first mix and heat the oil phase and emulsifier, then add the water phase, at a temperature of 65- Under the condition of 70°C, mix and discharge to obtain the product silk protein sunscreen.
[0036] Further, the oil phase includes the following...
Embodiment 1
[0041] Pretreatment of graphene oxide:
[0042] Mix graphene oxide and nano-inorganic powder at a mass ratio of 10:1-20:1, pour into deionized water that is 8-10 times the mass of graphene oxide, at an ultrasonic frequency of 45-65kHz and a temperature of 45-65 Under the condition of ℃, keep warm and ultrasonically disperse for 10-60min, then filter with suction, and wash the filter cake with deionized water for 3-5 times, then dry the washed filter cake at a temperature of 105-110 ℃ to constant weight, and discharge , to obtain pretreated graphene oxide; the nano-inorganic powder is nano-zinc oxide and / or nano-titanium dioxide;
[0043] Preparation of the water phase:
[0044] In parts by weight, 100-200 parts of water, 10-20 parts of glycerin, 8-10 parts of pretreated graphene oxide, 3-5 parts of dopamine, and 8-10 parts of silk protein are sequentially taken;
[0045] After mixing water, glycerin and silk protein, let it swell at room temperature for 8-24 hours, then pour...
Embodiment 2
[0050] Pretreatment of graphene oxide:
[0051] Mix graphene oxide and nano-inorganic powder at a mass ratio of 10:1-20:1, pour into deionized water that is 8-10 times the mass of graphene oxide, at an ultrasonic frequency of 45-65kHz and a temperature of 45-65 Under the condition of ℃, keep warm and ultrasonically disperse for 10-60min, then filter with suction, and wash the filter cake with deionized water for 3-5 times, then dry the washed filter cake at a temperature of 105-110 ℃ to constant weight, and discharge , to obtain pretreated graphene oxide; the nano-inorganic powder is nano-zinc oxide and / or nano-titanium dioxide;
[0052]Preparation of the water phase:
[0053] In parts by weight, 100-200 parts of water, 10-20 parts of glycerin, 8-10 parts of pretreated graphene oxide, 3-5 parts of dopamine, and 8-10 parts of silk protein are sequentially taken;
[0054] After mixing water, glycerin and silk protein, let it swell at room temperature for 8-24 hours, then pour ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com