Suspension acid thickening agent and preparation method thereof
A technology of thickening agent and suspending acid, which is applied in the direction of chemical instruments and methods, drilling compositions, etc., can solve the problems of low viscosity, easy agglomeration, poor dispersibility of thickened acid, etc., and achieve high viscosity and not easy agglomeration , The effect of slurry stabilization
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0038] A kind of suspending acid thickener, comprises following composition by weight percentage:
[0039] No. 3 white oil: 12 wt%,
[0040] No. 26 white oil: 10 wt%,
[0041] No. 100 white oil: 8 wt%,
[0042] No. 200 white oil: 10 wt%,
[0043] Organic bentonite: 6 wt%,
[0044] 100 mesh bentonite: 3 wt%,
[0045] 140 mesh kaolin: 9 wt%,
[0046] 160 mesh diatomaceous earth: 12 wt%,
[0047] 200 mesh fly ash: 9 wt%,
[0048] 95% ethanol: 3 wt%,
[0049] Thickener: 18 wt%.
[0050] Stir and mix the above-mentioned raw materials evenly in proportion, and the stirring time is 2 hours. After the stirring is completed, it is the product, code-named sample 1.
Embodiment 2
[0052] A kind of suspending acid thickener, comprises following composition by weight percentage:
[0053] No. 3 white oil: 19 wt%,
[0054] No. 26 white oil: 5 wt%,
[0055] No. 100 white oil: 6 wt%,
[0056] No. 200 white oil: 9 wt%,
[0057] Organic bentonite: 5 wt%,
[0058] 100 mesh bentonite: 7 wt%,
[0059] 140 mesh kaolin: 7 wt%,
[0060] 160 mesh diatomaceous earth: 7 wt%,
[0061] 200 mesh fly ash: 11 wt%,
[0062] 95% ethanol: 2 wt%,
[0063] Thickener: 22 wt%.
[0064] Stir and mix the above-mentioned raw materials evenly in proportion, and the stirring time is 2 hours. After the stirring is completed, it is the product, code-named sample 2.
Embodiment 3
[0066] A kind of suspending acid thickener, comprises following composition by weight percentage:
[0067] No. 3 white oil: 15 wt%,
[0068] No. 26 white oil: 13 wt%,
[0069] No. 100 white oil: 5 wt%,
[0070] No. 200 white oil: 8 wt%,
[0071] Organic bentonite: 3 wt%,
[0072] 100 mesh bentonite: 5 wt%,
[0073] 140 mesh kaolin: 6 wt%,
[0074] 160 mesh diatomaceous earth: 9 wt%,
[0075] 200 mesh fly ash: 12 wt%,
[0076] 95% ethanol: 1 wt%,
[0077] Thickener: 23 wt%.
[0078] Stir and mix the above-mentioned raw materials evenly in proportion, and the stirring time is 2 hours. After the stirring is completed, it is the product, code-named sample 3.
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
density | aaaaa | aaaaa |
shear viscosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com