A cat litter and range technology, applied in animal houses, applications, animal husbandry, etc., can solve the problems of uneven particles, large dust, poor water absorption and taste absorption, etc., to increase the contact area, reduce production costs, and improve viscosity. The effect of knot strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0066] The mass fraction ratio of Gorgon seed coat fragments, mint leaf fragments and soluble starch in the aggregate layer 2 is 2:1:6.
[0067] The particle diameter of the Gorgon seed coat fragment is equal to that of the mint leaf fragment, and both pass through a 100-mesh sieve.
[0068] The filler layer 3 includes Gorgon seed husk powder and soluble starch in a mass fraction ratio of 2:3.
[0069] The particle size of the Gorgon seed coat powder passes through a 150-mesh sieve.
[0070] The coating layer 4 is purified attapulgite clay powder.
[0071] The particle size of the attapulgite clay purified powder passes through a 180-mesh sieve.
[0072] The particle diameter of described cat litter 1 is at 2 millimeters.
[0073] The diameter of the aggregate layer 2 is 0.6 mm.
[0074] The thickness of the filler layer 3 is 0.5 mm.
[0075] The thickness of the cladding layer 4 is 0.2 mm.
[0076] Prepare a kind of method for cat litter as above, comprises the followin...
Embodiment 2
[0090] The mass fraction ratio of Gorgon seed coat fragments, mint leaf fragments and soluble starch in the aggregate layer 2 is 3:2:6.
[0091] The particle diameter of the Gorgon seed coat fragment is equal to that of the mint leaf fragment, and both pass through a 70-mesh sieve.
[0092] The filler layer 3 includes Gorgon seed husk powder and soluble starch in a mass fraction ratio of 1:3.
[0093] The particle size of the Gorgon seed coat powder passes through a 120-mesh sieve.
[0094] The coating layer 4 is purified attapulgite clay powder.
[0095] The particle size of the attapulgite clay purified powder passes through a 190-mesh sieve.
[0096] The particle diameter of described cat litter 1 is at 2.5 millimeters.
[0097] The diameter of the aggregate layer 2 is 0.6 mm.
[0098] The thickness of the filler layer 3 is 0.7 mm.
[0099] The thickness of the cladding layer 4 is 0.25 mm.
[0100] Prepare a kind of method for cat litter as above, comprises the follow...
Embodiment 3
[0114] The mass fraction ratio of Gorgon seed coat fragments, mint leaf fragments and soluble starch in the aggregate layer 2 is 4:2:5.
[0115] The particle diameter of the Gorgon seed coat fragment is equal to that of the mint leaf fragment, and both pass through a 90-mesh sieve.
[0116] The filler layer 3 includes Gorgon seed husk powder and soluble starch with a mass fraction ratio of 1.5:2.
[0117] The particle size of the Gorgon seed coat powder passes through a 120-mesh sieve.
[0118] The coating layer 4 is purified attapulgite clay powder.
[0119] The particle diameter of the attapulgite clay purified powder passes through a 200-mesh sieve.
[0120] The particle diameter of described cat litter 1 is at 3 millimeters.
[0121] The diameter of the aggregate layer 2 is 0.9 mm.
[0122] The thickness of the filler layer 3 is 0.8 mm.
[0123] The thickness of the cladding layer 4 is 0.25 mm.
[0124] Prepare a kind of method for cat litter as above, comprises the ...
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com