Expanded ceramisites prepared from residual sludge in combination with FCC spent catalyst and preparation method of expanded ceramisites
A technology of expanded ceramsite and waste catalyst, which is applied to clay products, ceramic products, and other household appliances. It can solve the problems of strong pollution, threats to the living environment, and low activity of spent catalysts, and achieve high economic value and reduced leaching rate. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0035] The ratio of excess sludge to catalyst is 3.5, and the mass of excess sludge is 1050g. Experimental conditions: particle size 200 mesh, add 5g NaOH, 2ml hydrogen peroxide. Appropriate amount of water; stirring speed: rotation 285 / min, revolution 125 / min; drying at 105°C for 4 hours, preheating in muffle furnace at 400°C for 20 minutes, and roasting at 1000°C for 10 minutes. The leaching toxicity of the obtained ceramsite is reduced from 2.3ppm to 0.15ppm; the apparent density is 1.9kg / m 3 .
Embodiment 2
[0037] The ratio of excess sludge to catalyst is 4, and the mass of excess sludge is 1200g. Experimental conditions: particle size 200 mesh, add 5g NaOH, 4ml hydrogen peroxide. Appropriate amount of water; stirring speed: rotation 285 / min, revolution 125 / min; drying at 105°C for 4 hours, preheating in muffle furnace at 400°C for 20 minutes, and roasting at 1100°C for 10 minutes. The leaching toxicity of the obtained ceramsite is reduced from 2.3ppm to 0.15ppm; the apparent density is 2.6kg / m 3 .
Embodiment 3
[0039] The ratio of excess sludge to catalyst is 4.5, and the mass of excess sludge is 1350g. Experimental conditions: particle size 200 mesh, add 5g NaOH, 6ml hydrogen peroxide. Appropriate amount of water; stirring speed: rotation 285 / min, revolution 125 / min; drying at 105°C for 4 hours, preheating in muffle furnace at 400°C for 20 minutes, and roasting at 1100°C for 10 minutes. The leaching toxicity of the obtained ceramsite is reduced from 2.3ppm to 0.15ppm; the apparent density is 3.0kg / m 3 .
PUM
Property | Measurement | Unit |
---|---|---|
Apparent density | aaaaa | aaaaa |
Apparent density | aaaaa | aaaaa |
Apparent density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com