Anti-ant environmental protection material and preparation method thereof
An environmentally friendly material and anti-ant technology, applied in antifouling/underwater coatings, paints containing biocides, coatings, etc., can solve the problems of reducing the service life of the house, not being widely used, and increasing the cost, and achieve the production cost. Low, significant anti-ant performance, the effect of prolonging the service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] An anti-ant environmental protection material, mainly made of the following raw materials in parts by weight: 30 parts of Portland cement, 20 parts of emulsion, 3 parts of water reducing agent, 10 parts of anti-termite agent, 3 parts of other additives and 40 parts of water;
[0023] Among them, the water reducer is made of sulfonated melamine formaldehyde resin; other additives are defoamers and thickeners;
[0024] The anti-termite agent is mainly made of the following raw materials in parts by weight: 10 parts of snake miemen extract, 10 parts of lip calyx peppermint extract, 10 parts of lavender extract, 20 parts of camphor leaf extract, 5 parts of carbamate and 4-chloro -5 parts of 2-phenylphenol; Its preparation method is:
[0025] S1: After removing impurities and cleaning the leaves of Shemimen, mint, lavender and camphor tree, they were minced and extracted with organic solvent ultrasonic waves, and then subjected to high-speed centrifugal filtration, clarifica...
Embodiment 2
[0031] An anti-termite environmental protection material, mainly made of the following raw materials in parts by weight: 45 parts of Portland cement, 30 parts of emulsion, 5 parts of water reducing agent, 15 parts of anti-termite agent, 4 parts of other additives and 60 parts of water;
[0032] Among them, the water reducer is mixed with sodium lignosulfonate and sodium sulfamate; other additives are mixed with antifungal agent and defoamer;
[0033] The anti-termite agent is mainly made of the following raw materials in parts by weight: 20 parts of snake miemen extract, 15 parts of lip calyx peppermint extract, 13 parts of lavender extract, 25 parts of camphor leaf extract, 6 parts of carbamate and 4-chloro -7 parts of 2-phenylphenol; Its preparation method is:
[0034] S1: After removing impurities and cleaning the leaves of Shemimen, mint, lavender and camphor tree, they were minced and extracted with organic solvent ultrasonic waves, and then subjected to high-speed centri...
Embodiment 3
[0040] An anti-ant environmental protection material, mainly made of the following raw materials in parts by weight: 60 parts of Portland cement, 40 parts of emulsion, 7 parts of water reducing agent, 20 parts of anti-termite agent, 5 parts of other additives and 80 parts of water;
[0041] Among them, the water reducing agent is a mixture of sulfonated melamine formaldehyde resin, sodium lignosulfonate and sodium sulfamate;
[0042] Other additives are antifungal agent, defoamer and thickener mixed;
[0043] The anti-termite agent is mainly made of the following raw materials in parts by weight: 30 parts of snake miemen extract, 20 parts of lip calyx peppermint extract, 15 parts of lavender extract, 30 parts of camphor leaf extract, 7 parts of carbamate and 4-chloro -10 parts of 2-phenylphenol; Its preparation method is:
[0044] S1: After removing impurities and cleaning the leaves of Shemimen, mint, lavender and camphor tree, they were minced and extracted with organic sol...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com