A technology of electric ignition and matches, applied in the direction of matches, etc., can solve the problems of polluting the environment, increasing the cost of raw materials, etc., and achieve the effect of no pollution, strong alcohol fixation ability, environmental protection and pollution-free price
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A preparation method for an electric ignition match, comprising the following steps:
[0023] 1) Weigh each substance separately according to the weight ratio of alcohol and thickener at 100:2, mix and stir with a mixer to form an alcohol gel-like viscous substance, insert one end of a thin wooden strip used as a matchstick and wrap it in alcohol Colloidal sticky thing; Described thickening agent is the mixture of carrageenan, sodium carboxymethyl cellulose, polyvinyl alcohol and water; Wherein the weight ratio of carrageenan, sodium carboxymethyl cellulose, polyvinyl alcohol and water 1:0.04:0.05:10, mix these components in proportion and heat to 70°C to dissolve completely to obtain the thickener;
[0024] 2) Insert one end of the matchstick covered with alcohol gel-like viscous substance into paraffin oil, and wrap the alcohol gel-like viscous substance with paraffin oil to form the primary drug head of the electric match;
[0025] 3) Weigh each substance according ...
Embodiment 2
[0028] A preparation method for an electric ignition match, comprising the following steps:
[0029] 1) Weigh each substance separately according to the weight ratio of alcohol and thickener at 100:0.3, mix and stir with a mixer to form an alcohol gel-like viscous substance, insert one end of a thin wooden strip used as a matchstick and wrap it in alcohol Colloidal viscous; the thickener is a mixture of carrageenan, sodium carboxymethyl cellulose, polyvinyl alcohol and water; wherein the weight ratio of alginate, sodium carboxymethyl cellulose, polyvinyl alcohol and water 1:0.005:0.1:5, mix these components in proportion and heat to 70°C to dissolve completely to obtain the thickener;
[0030] 2) Insert one end of the matchstick covered with alcohol gel-like viscous substance into paraffin oil, and wrap the alcohol gel-like viscous substance with paraffin oil to form the primary drug head of the electric match;
[0031] 3) Weigh each substance according to the weight ratio of...
Embodiment 3
[0034] A preparation method for an electric ignition match, comprising the following steps:
[0035] 1) Weigh each material separately according to the weight ratio of alcohol and thickener at 100:5, mix and stir with a mixer to form an alcohol gel-like viscous substance, insert one end of a thin wooden strip used as a matchstick and wrap it in alcohol Colloidal viscous; the thickener is a mixture of alginate, sodium carboxymethylcellulose, polyvinyl alcohol and water; wherein the weight ratio of alginate, sodium carboxymethylcellulose, polyvinyl alcohol and water 1: 0.08:0.01:30, mix these components in proportion and heat to 70°C to dissolve completely to obtain the thickener;
[0036] 2) Insert one end of the matchstick covered with alcohol gel-like viscous substance into paraffin oil, and wrap the alcohol gel-like viscous substance with paraffin oil to form the primary drug head of the electric match;
[0037] 3) Weigh each substance according to the weight ratio of sawdu...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com