Accelerating agent with low adding amount, and preparation process thereof
A technology of quick-setting agent and low dosage, which is applied in the field of quick-setting agent and its production process, which can solve the problems of increasing water-cement ratio, increasing construction water demand, and adverse effects on concrete strength, so as to achieve good strength and reduce construction needs. The effect of water volume
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Raw materials: 10kg of zinc sulfate, 10kg of hydrogen peroxide, 20kg of polyaluminum sulfate, 20kg of titanium slag, 45kg of vanadium slag, 25kg of soda ash and 15kg of dextrin.
[0014] Production process: After mixing zinc sulfate, hydrogen peroxide and polyaluminum sulfate, add 55% water, mix well, heat to 20-25°C, keep warm for 4.5h, add the remaining raw materials, mix well and heat to 40- Keep warm at 45°C for 1 hour, then add the remaining amount of water and mix well to obtain the finished product.
Embodiment 2
[0016] Raw materials: 15kg of zinc sulfate, 15kg of hydrogen peroxide, 22kg of polyaluminum sulfate, 22kg of titanium slag, 48kg of vanadium slag, 30kg of soda ash, 105kg of water and 20kg of dextrin.
[0017] Production process: After mixing zinc sulfate, hydrogen peroxide and polyaluminum sulfate, add 55% water, mix well, heat to 20-25°C, keep warm for 4.5h, add the remaining raw materials, mix well and heat to 40- Keep warm at 45°C for 1 hour, then add the remaining amount of water and mix well to obtain the finished product.
Embodiment 3
[0019] Raw materials: 5kg of zinc sulfate, 5kg of hydrogen peroxide, 18kg of polyaluminum sulfate, 18kg of titanium slag, 43kg of vanadium slag, 20kg of soda ash, 91kg of water and 10kg of dextrin.
[0020] Production process: After mixing zinc sulfate, hydrogen peroxide and polyaluminum sulfate, add 55% water, mix well, heat to 20-25°C, keep warm for 4.5h, add the remaining raw materials, mix well and heat to 40- Keep warm at 45°C for 1 hour, then add the remaining amount of water and mix well to obtain the finished product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com