Embodiment 1
[0030] A graphene amine-aldehyde resin for impregnation, used to produce impregnated film paper, its components include formaldehyde, melamine, water, urea, aldehyde absorbent, graphene, 906 triamine auxiliary agent, obtained through the following steps:
[0031] 1) Configure graphene amine-formaldehyde resin, add 100 parts by weight of 37%wt formaldehyde and 40 parts by weight of water into the reactor, heat the reactor to 20°C-30°C by turning on the steam, turn on the stirrer, and oxidize with 30% hydrogen The sodium solution adjusts the pH value to 8.5;
[0032] 2) Add 80 parts by weight of melamine, continue to heat up, and add 10 parts by weight of 906 triamine additive when the melamine turns clear;
[0033] 3) Continue to turn on the steam and heat the reactor to 90°C, stop the gas and keep it for 10 minutes, then heat up to 93°C-96°C for polycondensation reaction;
[0034] 4) When it is detected that the mixing ratio of water and mixture is 1:2.2, turn on the cooling ...
Embodiment 2
[0040] 1) Configure graphene amine-aldehyde resin, add 120 parts by weight of 37%wt formaldehyde and 45 parts by weight of water into the reactor, heat the reactor to 20°C-30°C by turning on the steam, turn on the stirrer, and oxidize with 30% hydrogen The sodium solution adjusts the pH value to 9;
[0041] 2) Add 80 parts by weight of melamine, continue to heat up, and add 10 parts by weight of 906 triamine additive when the melamine turns clear;
[0042] 3) Continue to turn on the steam and heat the reactor to 90°C, stop the gas and keep it for 10 minutes, then heat up to 93°C-96°C for polycondensation reaction;
[0043] 4) When it is detected that the mixing ratio of water and mixture is 1:2.3, turn on the cooling water to cool down;
[0044] 5) When the temperature is lowered to 85°C, 3 parts by weight of urea and 1.2 parts by weight of aldehyde absorbent are added;
[0045] 6) Add 0.05 parts by weight of graphene when the temperature is lowered to 60°C;
[0046] 7) Aft...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com