A kind of high-gloss and low-haze sprayable automotive protective coating and preparation method thereof
A protective coating and low haze technology, applied in the direction of coating, etc., can solve the problems of affecting the use effect and aesthetics, affecting the appearance of the car body, and the car's protection effect is small, so as to eliminate appearance defects, improve gloss, and reduce surface roughness degree of effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A high-gloss and low-haze sprayable protective coating for vehicles, comprising a base film layer and functional layers arranged on the upper and lower sides of the base film layer, in parts by weight, its raw material formula is as follows:
[0021] 1000 parts of C6-C8 aliphatic hydrocarbon with low boiling point, 1300 parts of vinyl silicone resin, 1000 parts of polyvinyl chloride resin, 1200 parts of metallocene linear low-density polyethylene, 1200 parts of vinegar-acrylic emulsion, diisooctyl succinate 50 parts of sodium sulfonate, 10 parts of PVC resin, and 80 parts of nano-alumina.
Embodiment 2
[0023] A high-gloss and low-haze sprayable protective coating for vehicles, comprising a base film layer and functional layers arranged on the upper and lower sides of the base film layer, in parts by weight, its raw material formula is as follows:
[0024] 1500 parts of C6-C8 aliphatic hydrocarbon with low boiling point, 1000 parts of vinyl silicone resin, 1500 parts of polyvinyl chloride resin, 800 parts of metallocene linear low density polyethylene, 1800 parts of vinegar-acrylic emulsion, diisooctyl succinate 35 parts of sodium sulfonate, 20 parts of PVC resin, 50 parts of nano aluminum oxide.
Embodiment 3
[0026] A high-gloss and low-haze sprayable protective coating for vehicles, comprising a base film layer and functional layers arranged on the upper and lower sides of the base film layer, in parts by weight, its raw material formula is as follows:
[0027] 1,200 parts of C6-C8 aliphatic hydrocarbons with low boiling point, 1,000 parts of vinyl silicone resin, 1,200 parts of polyvinyl chloride resin, 1,000 parts of metallocene linear low-density polyethylene, 1,500 parts of vinegar-acrylic emulsion, diisooctyl succinate 45 parts of sodium sulfonate, 15 parts of PVC resin, 60 parts of nanometer aluminum oxide.
PUM
Property | Measurement | Unit |
---|---|---|
haze | aaaaa | aaaaa |
gloss | aaaaa | aaaaa |
haze | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com