Steel pipe gypsum mortar and waste concrete combined column and preparation method thereof
A technology for waste concrete and waste concrete blocks, which can be applied to columns, piers, pillars, etc., and can solve problems such as poor strength, poor bonding strength between filling materials and steel pipes, and slow setting speed.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0018] refer to figure 1 As shown, the steel pipe gypsum mortar waste concrete composite column provided by the present invention comprises a steel pipe 1, a gypsum mortar 2 and a waste concrete block 3 filled in the steel pipe 1, the two ends of the steel pipe 1 are sealed by end plates, and the gypsum mortar 2 is made of water, gypsum and Sand composition, the ratio of water, gypsum and sand is 0.3:1:1-0.5:1:1, the greater the mixing water consumption, the lower the strength, the better the fluidity, and the gypsum mortar 2 is also added with a retarder, retarder The coagulant is citric acid, which is used to adjust the flocculation time of the gypsum mortar 2. The maximum diameter of the waste concrete block 3 is 1 / 4-1 / 3 of the diameter of the steel pipe 1, and the minimum diameter of the waste concrete block 3 is 20-30mm.
[0019] refer to figure 1 As shown, in order to increase the structural strength, there are many pairs of transverse reinforcement sockets 4 arranged a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com