Phosphorus-free scale and corrosion inhibitor containing fulvic acid and preparation method thereof
A phosphorus-free scale inhibition, fulvic acid technology, applied in chemical instruments and methods, descaling and water softening, water/sludge/sewage treatment, etc. Biodegradation and other problems, to achieve the effect of reducing environmental pollution, good stability and high flocculation ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] A preparation method of a phosphorus-free scale and corrosion inhibitor containing fulvic acid, the specific operation steps are as follows:
[0033] step 1,
[0034] Weigh 300g of scale inhibitor components, 300g of corrosion inhibitor components and 400g of deionized water;
[0035] Wherein, the antiscalant component of 300g is made up of the fulvic acid of 27% by mass percentage, the maleic acid-acrylic acid binary copolymer of 28%, the polyaspartic acid of 45%;
[0036] The corrosion inhibiting component of 300g is made up of the zinc sulfate of 30% by mass percentage, the imidazoline of polyoxyethylene naphthenate of 70%;
[0037] Step 2,
[0038] Add zinc sulfate to deionized water, stir fully to completely dissolve zinc sulfate, and obtain mixture A;
[0039] Step 3,
[0040] Add fulvic acid to mixture A and stir well to obtain mixture B;
[0041] Step 4,
[0042] Add maleic acid-acrylic acid binary copolymer and polyaspartic acid successively to mixture B,...
Embodiment 2
[0070] A preparation method of a phosphorus-free scale and corrosion inhibitor containing fulvic acid, the specific operation steps are as follows:
[0071] step 1,
[0072] Weigh 500g of scale inhibitor component, 400g of corrosion inhibitor component and 100g of deionized water;
[0073] Wherein, the antiscaling component of 500g is made up of the fulvic acid of 40% by mass percentage, the maleic acid-acrylic acid binary copolymer of 30%, the polyaspartic acid of 30%;
[0074] The corrosion inhibitor component of 300g is made up of the zinc sulfate of 40% by mass percentage, the imidazoline of polyoxyethylene naphthenate of 60%;
[0075] Step 2,
[0076] Add zinc sulfate to deionized water, stir fully to completely dissolve zinc sulfate, and obtain mixture A;
[0077] Step 3,
[0078] Add fulvic acid to mixture A and stir well to obtain mixture B;
[0079] Step 4,
[0080] Add maleic acid-acrylic acid binary copolymer and polyaspartic acid successively to mixture B, st...
Embodiment 3
[0109] A preparation method of a phosphorus-free scale and corrosion inhibitor containing fulvic acid, the specific operation steps are as follows:
[0110] step 1,
[0111] Weigh 200g of scale inhibitor components, 150g of corrosion inhibitor components and 650g of deionized water;
[0112] Wherein, the antiscaling component of 200g is made up of the fulvic acid of 25% by mass percent, the maleic acid-acrylic acid binary copolymer of 20%, the polyaspartic acid of 55%;
[0113] The corrosion inhibitor component of 300g is made up of the zinc sulfate of 55% by mass percentage, the imidazoline of polyoxyethylene naphthenate of 45%;
[0114] Step 2,
[0115] Add zinc sulfate to deionized water, stir fully to completely dissolve zinc sulfate, and obtain mixture A;
[0116] Step 3,
[0117] Add fulvic acid to mixture A and stir well to obtain mixture B;
[0118] Step 4,
[0119] Add maleic acid-acrylic acid binary copolymer and polyaspartic acid successively to mixture B, stir ...
PUM
Property | Measurement | Unit |
---|---|---|
scale inhibition rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com