Preparation method of salt containing compound components
A salt and ingredient technology, applied in the field of preparation of compound ingredient salt, can solve the problems of unsatisfactory content uniformity, prone to delamination, harm increase, etc., to avoid the adhesion of salt particles, not easy to delaminate, and to overcome adhesion. powerful effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0031] The embodiment of the present invention discloses a preparation method of composite salt, comprising the following steps:
[0032] (A) mixing and stirring the plant extract, plasticizer, lubricant and solvent to obtain a homogeneous dispersion;
[0033] (B) Utilizing a fluidized coating machine to wrap the dispersion on the surface of the sieved raw salt to obtain a composite salt;
[0034] Set the parameters of the fluidized coating machine, the negative pressure inside the machine is 200-500Pa, the air inlet temperature is 35-85°C, the raw salt temperature is 30-70°C, and the spray gun atomization pressure is 0.1-0.7Mpa.
[0035] The present invention is directed at the preparation method of the composite salt of mixed plant extracts. The invention realizes the coating of the raw material salt by controlling the appropriate parameters of the fluidized coating machine, ensures the uniformity of the particle size of the final product and the content of the plant extrac...
Embodiment 1
[0058] a) Pass 800g of edible salt through a 60-80 mesh sieve, and use the sieve for later use.
[0059] b) Dissolve 200g of seaweed extract, 10.5g of talcum powder, and 40g of "starch1500" (partially pregelatinized starch) in 560ml of distilled water, and stir the mixture at a low speed of 20rpm for 30 minutes with a stirring blade.
[0060] The seaweed extract is oligomeric alginic acid extracted from brown algae.
[0061] c) Add the salt in step a) into the equipment, turn on the bottom spray ring chassis fluidized coating machine, the negative pressure inside the machine is 200Pa, so that the salt becomes "boiling"; set the equipment inlet air temperature to 54°C, and the outlet air temperature 100°C, salt temperature 36°C (observed value), air intake 85m 3 / h, the air inlet humidity is 5%. When the salt reaches 36°C, start spraying, the spray gun atomization pressure is 0.1Mpa, and the control parameters are 5.1g / min~6.3g / min until the spraying ends. Close the equipmen...
Embodiment 2
[0064] a) Pass 800g of edible salt through a 30-60 mesh sieve, and use the sieve for later use.
[0065] b) 200g of seaweed extract (same as Example 1) was dissolved in 400ml of distilled water, and the mixture was stirred at a low speed of 50rpm by a stirring blade for 30 minutes.
[0066] c) Add the salt in step a) into the equipment, turn on the bottom spray ring chassis fluidized coating machine, the negative pressure inside the machine is 300Pa, so that the salt becomes "boiling"; set the equipment inlet air temperature to 65°C, and the outlet air temperature 100°C, salt temperature 46°C (observed value), air intake 100m 3 / h, the air inlet humidity is 8%. When the salt reaches 46°C, start spraying, and the control parameters are 5.1g / min~6.3g / min until the spraying ends. Close the equipment after 5 minutes of spraying, end the preparation process, and discharge the material.
[0067] d) Granule quality: moisture ≤ 0.3%. Particle size (0.15-0.85mm)>80%. Additive cont...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com