[0026] 1) Raw material formula
[0027] EGCG
0.5g
1.5g
Nano Titanium Dioxide
2.5g
0.5g
1.0g
Cayson
0.1g
Deionized water
93.9g
[0028] 2) Add the formula amount of nano-scale titanium dioxide, hyaluronic acid and propylene glycol into 30 ml of deionized water, stir and heat to 75-95°C. After the hyaluronic acid and propylene glycol are completely dissolved, keep it warm for 10-15 minutes to obtain the foundation solution;
[0029] 3) Take the formula amount EGCG and add 20 ml of deionized water, stir at 35-55°C until completely dissolved to obtain solution A;
[0030] 4) Take the formula amount of dipotassium glycyrrhizinate and add 44 ml of deionized water, and stir at 75-95°C until completely dissolved to obtain solution B;
[0031] 5) Bring the basic solution to 50-65°C, then add Caython according to the formula and stir evenl...
Embodiment 2
[0034] 1) Raw material formula
[0035] EGCG
1.0g
1.0g
Nano Titanium Dioxide
5.0g
hyaluronic acid
0.5g
2.0g
Cayson
0.2g
Deionized water
90.3g
[0036] 2) Add the formula amount of nano-scale titanium dioxide, hyaluronic acid and propylene glycol into 30 ml of deionized water, stir and heat to 75-95°C. After the hyaluronic acid and propylene glycol are completely dissolved, keep it warm for 10-15 minutes to obtain the foundation solution;
[0037] 3) Take the formula amount EGCG and add 20 ml of deionized water, stir at 35-55°C until completely dissolved to obtain solution A;
[0038] 4) Take the formula amount of dipotassium glycyrrhizinate and add 40 ml of deionized water, stir at 75-95°C until completely dissolved to obtain solution B;
[0039] 5) Bring the basic solution to 50-65°C, then add Caython according to the formula and stir evenly to...
Embodiment 3
[0042] 1) Raw material formula
[0043] EGCG
2.0g
0.5g
Nano Titanium Dioxide
10.0g
hyaluronic acid
1.5g
4.0g
Cayson
0.5g
Deionized water
81.5g
[0044] 2) Add the formula amount of nano-scale titanium dioxide, hyaluronic acid and propylene glycol into 30 ml of deionized water, stir and heat to 75-95°C. After the hyaluronic acid and propylene glycol are completely dissolved, keep it warm for 10-15 minutes to obtain the foundation solution;
[0045] 3) Take the formula amount EGCG and add 20 ml of deionized water, stir at 35-55°C until completely dissolved to obtain solution A;
[0046] 4) Take the formula amount of dipotassium glycyrrhizinate and add 32 ml of deionized water, stir at 75-95°C until completely dissolved to obtain solution B;
[0047] 5) Bring the basic solution to 50-65°C, then add Caython according to the formula and stir evenly t...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com