Pre-makeup solid water capable of improving makeup durability and preparation method of pre-makeup solid water
A solid water, long-lasting technology, applied in the direction of cosmetic preparations, dressing preparations, skin care preparations, etc., can solve problems such as spending a lot of time, distracting attention, and poor skin adhesion, and achieve protection from Invasive, skin-enhancing, skin-plumping effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] A pre-makeup solid water prepared according to the following steps:
[0019] 1) Each component is weighed according to the formula, and the formula includes each component in the following weight percentages, and the sum of the weight percentages of each component is 100%: glycerin 5%, cyclopentasiloxane and acrylic acid (ester) Polydimethylsiloxane copolymer (KP-545 produced by Shin-Etsu Japan) 0.3%, dioctyl carbonate 4%, cyclopentasiloxane 5%, phenoxyethanol and ethyl 0.1% hexylglycerin, 5% butanediol, 0.4% ammonium acryloyldimethyl taurate / VP copolymer, 0.01% sodium hyaluronate (produced by Shandong Freda), 0.01% essence, oat β-glucan Sugar 0.5%, water balance;
[0020] 2) Add water, butylene glycol, glycerin, sodium hyaluronate, and ammonium acryloyldimethyltaurate / VP copolymer into the water phase pot, stir to raise the temperature to 80 degrees Celsius, keep warm and stir for 20 minutes, and use it as the water phase for later use;
[0021] 3) Add dioctyl carbon...
Embodiment 2
[0025] A pre-makeup solid water prepared according to the following steps:
[0026] 1) Each component is weighed according to the formula, and the formula includes each component in the following weight percentages, and the sum of the weight percentages of each component is 100%: glycerin 10%, cyclopentasiloxane and acrylic acid (ester) Dimethicone Copolymer (KP-545 produced by Shin-Etsu Corporation) 1.0%, Dioctyl Carbonate 5%, Cyclopentasiloxane 5%, Phenoxyethanol and Ethylhexyl Glycerin 0.4%, Butylene Glycol 7%, Acryloyldimethyltaurate Ammonium / VP Copolymer 1%, Sodium Hyaluronate (produced by Shandong Freda) 0.2%, Essence 0.2%, Oat β-glucan 2%, water balance;
[0027] 2) Add water, butylene glycol, glycerin, sodium hyaluronate, and ammonium acryloyldimethyltaurate / VP copolymer into the water phase pot, stir to raise the temperature to 80 degrees Celsius, and keep stirring for 20 minutes;
[0028] 3) Add dioctyl carbonate, cyclopentasiloxane, cyclopentasiloxane and acrylic ...
Embodiment 3
[0032] A pre-makeup solid water prepared according to the following steps:
[0033] 1) Each component is weighed according to the formula, and the formula includes each component in the following weight percentages, and the sum of the weight percentages of each component is 100%: glycerin 8%, cyclopentasiloxane and acrylic acid (ester) Dimethicone Copolymer (KP-545 produced by Shin-Etsu Japan) 0.5%, Dioctyl Carbonate 6%, Cyclopentasiloxane 8%, Phenoxyethanol and Ethylhexyl Glycerin 0.8%, Butylene Glycol 10%, Acryloyldimethyltaurate Ammonium / VP Copolymer 0.8%, Sodium Hyaluronate (produced by Shandong Freda) 0.2%, Essence 0.2%, Oat β-glucan 0.9%, water balance;
[0034] 2) Add water, butylene glycol, glycerin, sodium hyaluronate, and ammonium acryloyldimethyltaurate / VP copolymer into the water phase pot, stir to raise the temperature to 80 degrees Celsius, and keep stirring for 20 minutes;
[0035] 3) Add dioctyl carbonate, cyclopentasiloxane, cyclopentasiloxane and acrylic ac...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com