Sodium cyanate gold leaching technology
A gold leaching and leaching technology with sodium cyanate is applied in the field of gold leaching with sodium cyanate to achieve the effects of reducing production cost, green and safe process, and simple operation.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0038] Firstly, the sulphur-containing gold ore ball mill is processed, and the fineness of the gold concentrate mineral material obtained after the treatment is -400 mesh accounting for 85%; then the slurry is adjusted so that the slurry-to-solid mass ratio is 2:1, and then it is added to the system in sequence Add 4kg / t of leaching aid Cao, 2kg / t of leaching aid Na 2 CO 3 , Adjust the pH of the system to 9.0, and finally add the gold leaching agent sodium cyanate with an amount of 0.5‰ of the weight of the gold concentrate. After leaching at 20-30°C for 10 hours, the gold leaching rate reaches 97.2%.
Embodiment 2
[0040] Firstly, the ball mill for sulfur-containing gold mines is processed, and the fineness of the gold concentrate obtained after the treatment is -400 mesh accounting for 90%; then the slurry is adjusted so that the slurry-to-solid mass ratio is 3:1, and then it is added to the system in turn Add 6kg / t of leaching aid Cao, 2kg / t of leaching aid Na 2 CO 3 , Adjust the pH of the system to 9.6, and finally add the gold leaching agent sodium cyanate, the amount is 3‰ of the weight of the gold concentrate, after leaching at 20-30℃ for 4 hours, the gold leaching rate reaches 98.7%.
Embodiment 3
[0042] Firstly, the gold oxide ore ball mill is processed, and the fineness of the gold concentrate mineral material obtained after the processing is -400 mesh accounting for 90%; then the slurry is adjusted so that the slurry-to-solid mass ratio is 4:1, and then it is added to the system in sequence 7kg / t of leaching aid Cao, 3kg / t of leaching aid Na 2 CO 3 , Adjust the pH of the system to 11.2, and finally add the gold leaching agent sodium cyanate, the amount of which is 5‰ of the weight of the gold concentrate. After leaching at 20-30°C for 10 hours, the gold leaching rate reaches 98.6%.
PUM
Property | Measurement | Unit |
---|---|---|
melting point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com