Acidified attapulgite clay
A technology of attapulgite clay and acidification treatment, which is applied in the direction of aluminum silicate and silicate, and can solve the problems of attapulgite clay colloidal performance degradation and other problems
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0027] Below in conjunction with embodiment the present invention will be further described:
[0028] 1. The acidified attapulgite clay ingredients are composed of the following components by weight percentage: acidified attapulgite clay semi-finished product 94.5%, instant sodium silicate 2.3%, polyvinyl alcohol 2%, hydroxypropyl methylcellulose 1% and Sodium Carbonate 0.2%.
[0029] 2. The production method of acidified attapulgite clay: input the acidified attapulgite clay ingredients into the mill for grinding, the particle fineness is ≤0.074 mm, and the powder after grinding is acidified attapulgite clay Clay finished.
[0030] 3. The production method of acidified attapulgite clay semi-finished products: (1) first input the naturally weathered attapulgite clay into the running mixer, and then slowly add dilute sulfuric acid into the naturally weathered attapulgite clay for acidification treatment ; (2) Extrude the attapulgite clay after the acidification treatment into...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com