Non-phosphorus corrosion and scale inhibitor for low-hardness water system industrial recycling cooling water
A technology of phosphorus-free corrosion and scale inhibitor, which is applied in the formulation of phosphorus-free corrosion and scale inhibitor, low hardness circulating cooling water, and phosphorus-free corrosion and scale inhibitor, can solve the problem that the effect of corrosion inhibitor cannot meet the field industrial application. , failure to form an effective system, etc., to avoid eutrophication and heavy metal pollution, to protect the environment, and to achieve good stability.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] 10% aqueous solution of low molecular weight tetrapolymer of AMPS, acrylic acid, maleic acid, sodium allyl sulfonate AMPS-AA-SAS-MA at a concentration of 30%; low molecular weight quaternary of AMPS-AA-SAS-MA The copolymer is commercially available, and its molecular weight is between 3000 and 5000; the concentration is 50% polyaspartic acid solution 15%, long chain alkyl sulfonate 10%, N-long chain alkyl amino carboxylate 5%, polyhydroxy carboxylate 5%, tungstate 3%, zinc salt 2%, pH stabilizer 1%, water 49%, add to the beaker in turn, stir well to get the required phosphorus-free corrosion and scale inhibition agent.
Embodiment 2
[0019] 15% aqueous solution of low molecular weight tetrapolymer of acrylic acid, maleic acid, sodium allyl sulfonate AMPS-AA-SAS-MA at a concentration of 30%; low molecular weight tetrapolymer of AMPS-AA-SAS-MA The molecular weight is between 3000 and 5000; the concentration is 50% polyaspartic acid solution 10%, long chain alkyl sulfonate 15%, N-long chain alkyl amino carboxylate 5%, polyhydroxy carboxylic acid Add 10% of salt, 2% of tungstate, 2% of zinc salt, 1% of pH stabilizer, and 40% of water into the beaker in turn, and stir evenly to obtain the required phosphorus-free corrosion and scale inhibitor.
Embodiment 3
[0021] 20% aqueous solution of low molecular weight tetrapolymer of acrylic acid, maleic acid, sodium allyl sulfonate AMPS-AA-SAS-MA with a concentration of 30%, low molecular weight tetrapolymer of AMPS-AA-SAS-MA The molecular weight is between 3000 and 5000; the concentration is 50% polyaspartic acid solution 10%, long chain alkyl sulfonate 5%, N-long chain alkyl amino carboxylate 10%, polyhydroxy carboxylic acid Add 10% of salt, 2% of tungstate, 2% of zinc salt, 1% of pH stabilizer, and 40% of water into the beaker in turn, and stir evenly to obtain the required phosphorus-free corrosion and scale inhibitor.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com