A production method and leather technology, applied in leather surface treatment, small raw hide/big raw hide/leather/fur treatment, small raw hide/large raw hide/leather skin/fur chemical treatment, etc., can solve the problem of being easily stained by dust and other pollutants Dirt, leather resistance is not up to, leather has no anti-fouling ability and other problems, to achieve the effect of maintaining the original luster, increasing the life of the leather, and strong anti-fouling ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] The invention provides a kind of antifouling, the production method of tensile leather, it comprises:
[0032] To prepare the leather, it is required to have a uniform thickness of 1.4~1.6 mm, the leather body is full, the fur is fine and soft, and the leather body is soft.
[0033] Primer coating process: Take 100 parts by mass of water, heat it to 10~25 degrees Celsius, add 20 parts by mass of penetrant, stir for 1~2 minutes, then add 100 parts by mass of discoloration wax, stir for 1~2 minutes, it is fully dissolved; The leather is laid flat on the conveyor belt of the roller coater, the roller speed is 24 rpm, the conveying speed of the conveyor belt is 0.1 m / s, the amount of paint is 30-40 grams per square foot, the roller coater is turned on, and the length is passed after coating. 20 meters, the conveying speed is 0.1 m / s, the baking temperature is 80~10 degrees Celsius, and the above rolling coating process is done once. Then: take 100 parts by mass of water, h...
Embodiment 2
[0040] The invention provides a kind of antifouling, the production method of tensile leather, it comprises:
[0041] To prepare the leather, it is required to have a uniform thickness of 1.4~1.6 mm, the leather body is full, the fur is fine and soft, and the leather body is soft.
[0042]Primer coating process: Take 100 parts by mass of water, heat it to 10~25 degrees Celsius, add 10 parts by mass of penetrant, stir for 1~2 minutes, then add 100 parts by mass of discoloration wax, stir for 1~2 minutes, it is fully dissolved; The leather is laid flat on the conveyor belt of the roller coater, the roller speed is 24 revolutions per second, and the conveying speed of the conveyor belt is 0.08 m / s. The roller coater is turned on and the coating amount is 30-40 grams per square foot. After coating, pass the length 20 meters, the conveying speed is 0.08 m / s, and the baking temperature is 80-10 degrees Celsius. The above rolling coating process is carried out once. Then: take 100 p...
Embodiment 3
[0049] The invention provides a kind of antifouling, the production method of tensile leather, it comprises:
[0050] To prepare the leather, it is required to have a uniform thickness of 1.4~1.6 mm, the leather body is full, the fur is fine and soft, and the leather body is soft.
[0051] Primer coating process: Take 100 parts by mass of water, heat it to 10~25 degrees Celsius, add 20 parts by mass of penetrant, stir for 1~2 minutes, then add 100 parts by mass of discoloration wax, stir for 1~2 minutes, it is fully dissolved; The leather is laid flat on the conveyor belt of the roller coater, the roller speed is 24 rpm, the conveying speed of the conveyor belt is 0.1 m / s, the amount of paint is 30-40 grams per square foot, the roller coater is turned on, and the length is passed after coating. 20 meters, the conveying speed is 0.1 m / s, the baking temperature is 80~10 degrees Celsius, and the above rolling coating process is done once. Then: take 100 parts by mass of water, h...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com